Steel grade: S275M
Number: 1.8818
Standard: EN 10025-4:2004, European standard for hot-rolled structural steel. Part 4 – Technical delivery conditions for thermomechanical rolled weldable fine grain structural steels. Steels specified in this standard are intended for use in heavily loaded parts of welded structures such as, bridges, flood gates, storage tanks, water supply tanks, etc., for service at ambient and low temperatures.
Welding: The fine-grain structural steel grades of this series can be perfectly welded both manually and using automatic equipment by means of all known welding processes, not least due to their reduced carbon content and the low carbon equivalent value.
Category: Steel Round Bar
S275M Chemical information, Mechanical properties Physical properties, Heat treatment, and Micro structure. It also contains the use of EN/S275M, such as it is commonly used in bars, sheet, plates, steel coils, steel pipes, forged and other materials application. Is a technical delivery conditions for thermomechanical rolled weldable fine grain structural steels. S275M steel plate/sheet belongs to thermomechanical rolled weldable fine grain structural steels, equivalent grades of grade of S275M steel is Germany StE285TM, DIN StE285TM, Italy FeE275KGTM, UNI FeE275KGTM.| EN/S275M Standard Number: | ||||||||||||
| ITEM | Standard Number | Descriptions | ||||||||||
| ||||||||||||
| Chemical | Min.(%) | Max.(%) | ||||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | V | Ta | |||
| 0.13 | 0.50 | 1.50 | 0.035 | 0.030 | 0.30 | 0.20 | ||||||
| W | N | Cu | Co | Pb | B | Nb | Al | Ti | Other | |||
| Euronorm Structural steel, EN S275M/1.8818 | ||||||||||||
| ||||||||||||
| Tensile strength | 115-234 | σb/MPa | ||||||||||
| Yield Strength | 23 | σ 0.2 ≥/MPa | ||||||||||
| Elongation | 65 | δ5≥ (%) | ||||||||||
| ψ | – | ψ≥ (%) | ||||||||||
| Akv | – | Akv≥/J | ||||||||||
| HBS | 123-321 | – | ||||||||||
| HRC | 30 | – | ||||||||||
| ||||||||||||
| Tensile strength | 231-231 | σb/MPa | ||||||||||
| Yield Strength | 154 | σ 0.2 ≥/MPa | ||||||||||
| Steel GradesEN S275M/1.8818 Chemical information,Mechanical properties Physical properties, Mechanical properties, Heat treatment, and Micro structure | ||||||||||||
| Elongation | 56 | δ5≥(%) | ||||||||||
| ψ | – | ψ≥(%) | ||||||||||
| Akv | – | Akv≥/J | ||||||||||
| HBS | 235-268 | – | ||||||||||
| HRC | 30 | – | ||||||||||
| EN S275(1.8818) Heat Treatment Regime | ||||||||||||
| Annealing | Quenching | Tempering | Normalizing | Q & T | ||||||||
| √ | √ | √ | √ | √ | ||||||||
| ||||||||||||
| Product type | Products | Dimension | Processes | Deliver Status | ||||||||
| Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID- WASHED, Shot Blasting | ||||||||
| Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, | ||||||||
| Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot- Rolled | Annealed, Solution and Aging, Q+T, ACID- WASHED, Shot Blasting | ||||||||
| Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID- WASHED | ||||||||
| We can produce Structure Steel the specifications follows: | ||||||||||||