S355J2+N Steel Plate Description

Being an unalloyed carbon mild steel it is supplied to customers in hot rolled condition. S355J2 N plates are welder friendly, high tensile strength and low carbon structural steel that is readily available to customers in weldable form. It has excellent cold forming properties and plates are often produced using killed steel process and exported to customers in controlled rolling or normalized condition. Here the symbol S is used for structural steel and JR symbol is used for temperature impact test. Furthermore, the raw material used for manufacturing these plates is well inspected and tested by inspection agencies and quality experts.

Well, if we talk about plate’s specification and standard, these plates are manufactured in accordance with both national and international standard and specification including ASTM, ASME, and API standard. These plates are specialized with shim sheet, BQ profile and perforated sheets. The size of these plates varies from 0.5mm to 200mm; thickness varies from 1000mm to 2500mm whereas its width varies from 2500mm to 12500mm. Moreover, these plates are even available to customers as per their needs and demand.

Category:
Offshore and Structural Steel Plates Suppliers in s355J2+N for Construction Steel Application

Manufacturer, Importer, Stockholder, Distributor, Suppliers and Exporters of S355J2+N EN10025-2 Steel Plates in China, Large stocks of plates certified to S355J2+N EN10025-2 are held in our warehouse and processing facilities

S355J2+N is the most common high strength steel for construction that we sell. It is a non-alloy structural steel to EN10025-2 2004. With its increase yield strength of S355 MPa over other construction steels such as S275 and S235 it is an excellent choice for delivering critical components or major structural members. It is also the modern equivalent of the EN10025 1990 S355J2G3.

As an unalloyed low carbon mild steel grade S355 is supplied in the hot rolled condition. The S355 steel specifications are high yield non alloy steels. First specified in the European EN10025 standard and later published by the British Standards Institure (BSI) as BS EN 10025 S355, S355J2 and S355J2+N. These standards superceded the BS4360 grades. The average minimum yield for this material is 355 N/mm2, hence the name S355. S355 offers high yield and tensile strength with a minimum yield strength of 355 N/mm², a structural grade steel which is widely used in engineering and construction industries, can be supplied with a variety of treatments and test options to ensure that it is a highly usable steel in your various projects.

S355J2+N is welder-friendly, low carbon, high tensile strength structural steel, can be readily welded to other weldable steel. For its low carbon equivalent, it possesses good cold-forming properties. The plate is produced by fully killed steel process and supplied in a normalized or controlled rolling condition.
S355J2+N and S355J2G3 are the same steel grades as both grades delivery condition are normalized. G3 and N stand for normalized.

S355J2+N and S355J2G3 are the same steel grades as both grades delivery condition are normalized. G3 and N stand for normalized.

S symbol for Structural Steel

JR symbol 20 temperature impact test

J0 symbol 0 temperature impact test

J2 symbol -20 temperature impact test

We can supply S355J2+N EN10025-2 Offshore and Structural Steel Plates:

Thickness from 5mm to 200mm
Width: from 1,500mm to 2,500mm
Length: from 6,000mm to 12,000mm

S355 Specification

  • BS EN 10025
  • S235, S275, S355, S420, S460, S690, S890, S960
  • BS EN 10225
  • S355, S420, S460
  • API 2H Gr50
  • ASME/ASTM SA/A 36, 283 Gr C, 285 Gr C, 572 Gr 50

Technical Features

  • Certified in accordance with EN 10204 3.2: ABS
  • Normalised, fully killed, fine grain, vacuum degassed
  • Sulphur content restricted to 0.005% maximum
  • Impact tested
  • Through thickness tested
  • Ultrasonically tested

Chemical Properties of S355J2+N Steel Plates

DINASTMENJISChemical CompositionC.E.
CSiMnCrMoNiVWSPCU
17100St52-3NA572-5010025-2:2004S355J2+NG3106SM490YBmax0.22max0.55max1.60–––––max0.035max0.035–max0.047

Mechanical properties of grade S355 J2+N (1.0038(dubl))

Thickness (mm)Yield Strength Reh min (N / mm²)Tensile Strength Rm min (N / mm²)Elongation A5 min (%)Impact Values Charpy-V-Notch Longitudinal Average from 3 Speimens Thk. >10<150mm.
3<thk<100315-355490-630max 2227 Joules at -20 C

Application of S355J2+N Steel Plates

  • ship building
  • Structural application in freight cars, transmission towers, dump trucks, cranes, trailers
  • construction,
  • mechanical manufacturing,
  • oil and gas platforms
  • power plant
  • palm oil equipments and machineries

S355J2+N EN 10025-2 Structural Steel Plate Packing

S355J2+N EN 10025-2 Structural Steel Plate is sleeved into plastic bag individually, pieces wrapped with water-proof material, bundled with nylon rope. Clear labels are tagged on the outside of the package for easy identification of the quantity and product I.D. Great care is taken during operation and transportation. S355J2+N EN 10025-2 Structural Steel Plate packing will be according to international standard in bundles strapped by strips then into containers to avoid any damage.

Delivery: Within 10-25 days or asap if we have enough stock

Types of Packaging:

  • – Bundles (hexagonal)
  • – Wooden Boxes
  • – Crates (steel/wooden)
  • – Special crates for U-Bend tubes with each radius separated
  • – Packaging for S355J2+N EN 10025-2 Structural Steel Plate EN10025-6 as per customer’s requirements

Special Features:

  • – Each bundle covered with plastic for protection against extreme weather.
  • – End of S355J2+N EN 10025-2 Structural Steel Plate protected by plastic Strip.
  • – Bundles strapped with plastic strips.
  • – Each radius of U-Bend tube separated by a separator.
  • – Packaging list (laminated) placed with box/crate.

S355J2+N EN 10025-2 Structural Steel Plates, Sheet, Slabs Sizes Available in Stock with Price S355J2+N EN 10025-2 Structural Steel Plate Sizes Available in Stock with Price

  • 0.2 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 0.3 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 0.4 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 0.8 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 1 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 1.65 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 2.11 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 3.1 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 04 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 05 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 06 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 08 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 10 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 12 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 15 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 16 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 18 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 20 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 22 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 25 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 28 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 30 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 32 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 35 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 36 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 38 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 40 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 42 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 45 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 50 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 52 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 60 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 62 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 65 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 70 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 80 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 90 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 100 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 110 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 120 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates
  • 120 MM THICKNESS x WIDTH1000 MM / 1250 MM / 1500 MM / 2000 MM / 2500 MM X LENGTH 1000 MM / 2500 MM / 3000 MM / 6000 MM / COIL CUT in S355J2+N EN 10025-2 Structural Steel Plates, Pressure Vessel Steel Plates

We export S355J2+N EN 10025-2 Structural Plates to Saudi Arabia, Iran, Iraq, United Arab Emirates, Qatar, Bahrain, Oman, Kuwait, Turkey, Egypt, Yemen, Syria, Israel, Jordan, Cyprus, Singapore, Malaysia, Indonesia, Thailand, Vietnam, South Korea, Japan, Sri Lanka, Maldives, Bangladesh, Mayanmar, Taiwan, Cambodia, Argentina, Bolivia, Brazil, Chile, Venezuela, Colombia, Ecuador, Guyana, Paraguay, Uruguay, United States of America, Canada, Mexico, Panama, Costa Rica, Puerto Rica, Trinidad And Tobago, Jamaica, Bahamas, Denmark, Russia, Norway, Germany, France, Italy, United Kingdom, Spain, Ukraine, Netherland, Belgium, Greece, Czech Republic, Portugal, Hungary, Albania, Austria, Switzerland, Slovakia, Finland, Ireland, Croatia, Slovenia, Malta, Nigeria, Algeria, Angola, South Africa, Libya, Egypt, Sudan, Equatorial Guinea, The Republic of Congo, Gabon, Europe, Africa, Asia, North America, South America, Middle East, Far East.etc.