Japan JFE steel profile

JFE Steel has a history of 90 years and is one of the top 10 steel companies in the world.

Based on its experience, research and development, JFE steel has made unremitting efforts to improve the equipment, increase the variety and enrich the quality management every year to meet the requirements of our customers.

In Japan JFE steel with three of the world’s most advanced medium plate factory, can manufacture 5350 mm wide and 360 mm thick medium plate products, such as high strength steel, wear-resistant steel, low temperature steel plate, boiler, pressure vessel steel plate, nickel high class atmosphere corrosion resisting steel plates, stainless steel plate, all kinds of composite steel plate, etc., more than millions of tons of production.

JFE Wear-resistant steel plate series

  • EH-C340, C400, C450, C500, C550
  • EH-C400LE, C450LE, C500LE

JFE High strength steel plate series

  • HITEN780S, 780LE
  • HITEN980S
  • HYD960LE

Category: Tag:

Lion metal is a leading wholesaler vendor, merchant, and exporter of JFE EH C400 Plates.

We also manufacture all the household stainless steel, high nickel alloys, and carbon steel C400 Plates are designed with a chemical composition like carbon, chromium, boron, molybdenum, manganese, phosphorous, silicon, nickel, and sulfur.

Also, these plates are made with mechanical properties such as yield strength, tensile strength, elongation, and longitudinal degrees.

JFE EH C400 plates include some of the specifications such as heat treatment, material types, Brinell hardness, and various grades.

C400 plates are applicable in many industries like machine building, lifting & mobile equipment, stone & iron chutes, framework structures, pylons & wearing plates, containers, truck frames, rail cars, crane booms, anti-drill plates like tumbling machine, shot blasting equipment, security doors, and stone crusher.

JFE EH C400 Steel Plates are also helpful in some purposes like dump truck bodies, loading buckets, bulldozers, and conveyors. This plate has found various applications like material and important parts of building & bridge construction, transport, and mining types of machinery.

EH C400 plates are precisely suitable for extreme atmosphere with high toughness, low temperatures, and resistant from high impact conditions of the plate. These plates are helpful in abrasion resistance, workability, and weldability.

These plates are also resistant to the safety of welded joints, and weld cracking. C400 is developed with the highly resistant from abrasion as compared to C500 plates.

JFE EVERHARD C400 Plates are mainly considered for the low-temperature toughness. These products are long-lasting as well as increase the formability and higher abrasion resistant plates.

Brinell hardness at the plate makes the plate low-temperature toughness. EH C400 plates are extremely more abrasion resistant than the regular steels. They are lighter in weight and contribute to the atmosphere.

These plates are useful in extreme cold conditions. These plates even enable low welding temperature craking.

JFE EH C400 Plates undergo many tests after production such as hydrostatic test:

Intragranular test, mechanical tests, Charpy test, hardness test, chemical test, tensile test, destructive test, flaring test, flattening test, Spectro test, blaze test, corrosion test, ultrasonic test, radiography test, pitting resistance test and many more.

JFE EH C400 Plate Specification :

  • Item: Abrasion Resistant Plate
  • Thickness : 5 – 50.8, 50.9 – 101.6
  • Length : 1,0000mm to 12,000mm
  • Width : 500mm to 3000mm
  • Surface : Tempering, Quenched, Normalized.
  • Certificates : ISO9001:2000
  • Production : Hot-Rolled (HR) / Cold-Rolled (CR)
  • Applications : concrete industry, metallurgy, fan industry, coal industry, mining machinery, construction machinery,etc.
  • Heat treatment : Controlled heat treatment

JFE EH C400 PLATES CHEMICAL COMPOSITION

GradeCSiMnPSCrMoVTiBCeq**
JFE EH C4000.20 max––––0.40 – 1.200.50 max–0.020 max.0.004 max.–

JFE EH C400 PLATES MECHANICAL PROPERTIES

Brand nameThickness(mm)Brinell hardness [guaranteed] (29.42 kN) Average of 5 pointsCharpy impact properties (2mmV)Ceq (%)**
[guaranteed]
Test temperature [guaranteed] (C°)Charpy absorbed energy (J) [guaranteed]*
EVERHARD-C4505 – 101.6450±25–––