Q355 Steel Description

Q355 is a kind of steel. It is a kind of low alloy high strength structural steel, widely used in Bridges, vehicles, ships, construction, pressure vessels, special equipment, etc., where “Q” means yield strength, 355 means the yield strength of this steel is 355MPa, and the yield value will decrease with the increase of the thickness of the material.

Chemical composition:

C: 0.24, Si: 0.55, Mn: 1.60, P: S: 0.035, 0.035, Cr: 0.30, Ni: 0.30, Cu: 0.40

Category:
Q355 steel is a Chinese low alloy high strength structural steel, which replaced Q345, the material density is 7.85 g/cm3. According to GB/T 1591 -2018, Q355 has 3 quality levels: Q355B, Q355C and Q355D. “Q” is the first letter of Chinese Pinyin: “qu fu dian”, which means Yield Strength, “355” is the minimum value of yield strength 355 MPa for steel thickness ≤16mm, and tensile strength is 470-630 Mpa.

Datasheet and Specification

The tables below shows the Q355 material datasheet and specifications such as chemical composition, and mechanical properties.

Q355 Steel Chemical Composition (Hot rolled)

Steel GradeQuality GradeC % (≤)Si % (≤)Mn (≤)P (≤)S (≤)Cr (≤)Ni (≤)Cu (≤)N (≤)
Q355Q355B0.240.551.60.0350.0350.300.300.400.012
Q355C0.200.0300.0300.012
Q355D0.200.0250.025–

Carbon Equivalent (CEV)

Based on smelting analysis, steel delivered in hot rolled state.

CEV (Mass fraction ≤%); Nominal thickness or diameter (d)
Steel GradeQuality Grade≤ 3030 < d ≤ 6363 < d ≤ 150150 < d ≤ 250250 < d ≤ 400
Q355Q355B0.45 (CEV)0.470.470.49–
Q355C–
Q355D0.49

Q355 Mechanical Properties (Hot rolled)

Notes:

  • 1 MPa = 1 N/mm2
  • 1 GPa = 1 kN/mm2
Yield Strength (≥N/mm2), Thickness or Dia. (d) in mm
Steel GradeQuality Leveld≤1616< d ≤4040 < d ≤6363 < d ≤ 8080< d ≤ 100100< d≤ 150150 < d≤ 200200 < d ≤ 250250 < d ≤ 400
Q355Q355B355345335325315295285275–
Q355C–
Q355D265
Tensile Strength (N/mm2), Dia. (d) mm
Steel GradeQuality Leveld≤100100 < d ≤ 150150 < d ≤ 250250 < d ≤ 400
Q355B,C,DQ355B470 – 630450 – 600450 – 600–
Q355C–
Q355D450 – 600

Q355 Steel Elongation

Dia. (d) mm; Elongation (%)
Sample directiond≤4040 < d ≤ 6363 < d ≤ 100100 < d ≤ 150150 < d≤ 200250 < d ≤ 400
Horizontal201918181717
Vertical222120181717

Charpy Impact

Charpy (V-notch) impact test temperature and impact absorption energy (KV2/J).

QualityTemperatureLongitudinal Impact Energy (J), ≥Transverse Impact Energy (J), ≥
Q355B20 ℃3427
Q355C0 ℃3427
Q355D-20 ℃34 (for thickness ≥250mm)27 (for thickness ≥250mm)

Features and Applications

Q355 steel has good mechanical properties, good weldability, hot and cold processing properties and corrosion resistance. Can be used to manufacture ships, boilers, pressure vessels, petroleum storage tanks, bridges, power station equipment, lifting transport machinery and other higher load welded structural parts.

Q355 Steel Equivalent Grade

Q355 carbon steel equivalent to European EN (German DIN EN, British BSI, French NF…) and ISO standard.

ChinaISOEuropean Union
StandardGradeStandardGradeStandardGrade (Material Number)
GB/T 1591 -2018Q355BISO 630-2S355BEN 10025-2S355, S355JR (1.0045)
Q355CS355CS355J0 (1.0553)
Q355DS355DS355J2 (1.0577)