QAL9-2 Copper Description

QAl9-2 aluminum bronze, with high strength, corrosion resistance in the atmosphere, fresh water and sea water is very good, can be welding and gas welding, not easy to braze, in hot and cold state pressure workability is good. Used to make springs and other corrosion resistant components, such as worm gear.

Basic information

Material name: Aluminum bronze drawing Rod (hard,5 ~ 40mm)

Brand name:

Standard: GB/T 4423-1992

Category:

QAL9-2 Plate/Sheep

This QAL9-2 alloy has higher mechanical properties , and with high mechanical properties, good wear properties and corrosion resistance, easy to machining, brazing and welding performance is good, small shrinkage coefficient, non-magnetic

Thickness : 3.0-25 MM

Length : ≤2000 MM

Width : ≤1000 MM

MOQ : 1 MT

 

PROPERTIES

QAL9-2 Chemical Composition

 

Alloy

Chemical Composition

Al

Mn

cu

QAl9-2

8.0-10.0

1.2-2.5

Rem

QAL9-2 Specification

Alloy

process

Size(mm)

Thickness

Width

Length

QAl9-2

Hot rolling

8.0-25

≤1000

≤2000

Cold rolling

3.0~12

≤1000

≤2000

QAL9-2 Mechanical Properties

Alloy

Temper

Tensile Strength(Mpa)

Elongation%

Hardness(HV)

QAl9-2

R

≥440(TH≤14mm)

A11.3≥15

–

M

≥295

≥35

–

Y

≥585

≥5

–

FEATURES

1) Good wear resistance

2) Excellent corrosion resistance

3) High resistance to high temperature, high pressure

4) Hot Forging performance

5) Good cutting performance

Thick plate/sheet

QAL9-2 PIPE

This alloy has higher mechanical properties , and with high mechanical properties, good wear properties and corrosion resistance, easy to machining, brazing and welding performance is good, small shrinkage coefficient, non-magnetic

Length : 500-6000 MM

OD : 90-250 MM

WT : 5-50 MM

MOQ : 1 MT

PROPERTIES

qal9-2-pipe

Chemical Composition

Alloy

Chemical Composition

Al

Mn

Cu

QAl9-2

8.0-10.0

1.2-2.5

Rem

Product

Alloy

shape

Temper

Size

OD.

WT.

Length (mm),max.

Extruded pipe

QAl9-2

round

R

90-250

5-50

L500-6000

FEATURES

1) Good wear resistance

2) Excellent corrosion resistance

3) High resistance to high temperature, high pressure

4) Hot Forging performance

5) Good cutting performance

Extruded pipe/tube

QAL9-2 pipe

TYPICAL USES

High strength, wear resistant parts, such as bearings, bushings, gear, turbine, etc.;Can also be made to take over the mouth, flange, oblate rocker arm, support, etc

QAL9-2 ROD

This alloy has higher mechanical properties , and with high mechanical properties, good wear properties and corrosion resistance, easy to machining, brazing and welding performance is good, small shrinkage coefficient, non-magnetic

qal9-2 bar

Length : 500-5000MM

OD : 10-200 MM

MOQ : 1MT

 

PROPERTIES

Chemical Composition

Alloy

Chemical Composition

Al

Mn

cu

QAl9-2

8.0-10.0

1.2-2.5

Rem

QAL9-2 Specification

Product

Alloy

shape

Temper

Size

OD.

Length (mm),max.

Extruded rod

QAl9-2

round

R

15-200

OD≤50 L1000-5000

OD>50-70 L500-5000
OD>75-120 L500~4000

OD>120 L300~4000

square ,

hexagonal

15-60

Drawn rod

Round,

square ,

hexagonal

Y

10-40

OD≤50 L1000-5000

OD>50-85 L500-5000

 

FEATURES

1) Good wear resistance

2) Excellent corrosion resistance

3) High resistance to high temperature, high pressure

4) Hot Forging performance

5) Good cutting performance

Extruded rod/bar

Drawn rod/pipe

QAL9-2 ROD copper

Please contact one of our knowledgeable sales staff to help you with your Copper needs.

REQUEST A QUOTE

* Required Fieds|We will reply you in 24 hours

You can contact us by E-mail or other ways.We will respond You in 24hours.