Nimonic 80 Definition
Nimonic 80A is a nickel-based superalloy composed of Ni-Cr. It has good strength and excellent corrosion resistance and oxidation resistance at high temperature. These advantages enable the Nimonic 80A to be used in a wide range of applications such as aerospace, power plants, and transportation.
Nimonic 80A Physical performance
Mass susceptibility: 5.85×10-6 at 1000 Gauss
Volume susceptibility: 4.78×10-5 at 1000 Gauss
Density: 8.19 g/cm3
Melting point: 1320-1365 ℃
Nickel Alloy 80A / Nimonic 80A®
Nimonic 80A Technical Data Sheet
Alloy 80A (Nimonic® alloy 80A) is a wrought, age-hardenable nickel-chromium alloy. Nimonic 80A is similar to alloy 75 but made precipitation hardenable by additions of aluminium and titanium. Alloy 80A has good corrosion and oxidation resistance and high tensile and creep-rupture properties at temperatures to 815ºC (1500ºF). Vacuum refined versions are also available. Alloy 80A is used for gas-turbine components (blades, rings, discs), bolts, tube supports in nuclear generators, exhaust valves in internal combustion engines and has many other offshore/marine, automotive and electrical applications.
Nimonic 80A Chemical Composition Limits
| Weight % | Ni | Cr | Ti | Al | C | Si | Cu | Fe | Mn | Co | B | Zr | S |
| Alloy 80A | Bal | 18.0-21.0 | 1.8-2.7 | 1.0-1.8 | 0.10 max | 1.0 max | 0.2 max | 3.0 max | 1.0 max | 2.0 max | 0.008 max | 0.15 max | 0.015 max |
Nimonic 80A Typical Mechanical Properties
| Material | Condition | Ultimate Tensile Strength ksi | Yield Strength ksi | Elongation on 4D (min) | Hardness min |
| Alloy 80A | Solution Annealed & Precipatation Treated (aged) | 145 | 90 | 20 | 300 HV |
Nimonic 80A Availability
Alloy 80A is available in Round Bar, Flat Bar, Rod, Tube, Plate, Sheet, Strip, Forging Stock and Wire. For all stock availability contact Sales.
Nimonic 80A Specifications
| Alloy 80A Rod, Bar, Wire and Forging Stock | BS 3076 HR1, ASTM B 637, AECMA PrEn2188, AECMA PrEn2189, AECMA PrEn 2190, AECMA PrEn 2396, AECMA PrEn2397, AIR 9165-37 |
| Alloy 80A Plate, Sheet and Strip | BS HR 201, AECMA PrEn2191 |
| Alloy 80A Pipe and Tube | BS HR 401 |
| Alloy 80A Other | BS HR 601, BS HR1, DIN 17742, AFNOR NC 20TA, UNS N07080, Werkstoff Nr 2.4952, Werkstoff Nr 2.4631, NIMONIC 80a (trademark), MSRR 7095 and MSRR 7011, MSRR 7013, HR201, HR401, HR601, NA20, VAT80A |