Data Table for: Carbon steel: 17NiCrMo6-4
Production specifications: Steel plate, Sheet, Coil, Flat bar, Round bar, Strip steel, wire,All kinds of forgings.
Mchining: Turning, Milling, Grinding
Deep hole drilling: length max 9.8 meters.
Range of work
- Round bar steel: 1mm to 2000mm
- Square-shape steel: 10mm to 1000mm
- steel Plate/sheet:0.08mm to 800mm
- Width: 10mm to 1500mm
- Lenth: We can supply any lenth based on the customer’s requirement.
- Forging: Shafts with flanks, tubes, slugs, donuts, cubes, other shapes
- Tubings: OD: φ4-410 mm, with wall thickness ranging from 1-35 mm.
Heat treatment:
Normalizing, Annealing, Tempering, Quenching, Hardening and tempering, Seasoning, Surface hardening, Carburizing
Category: Steel Round Bar
Tags: 1.6566 17NiCrMo6-4 18NCD6 18NiCrMo5 4317 817M17
17NiCrMo6-4 Steel Round Bar

17NiCrMo6-4 (UNI EN 10084) IS THE NEW DESIGNATION OF 18NiCrMo5 (UNI 7846). IT IS THE MOST COMMON CASE-HARDENING STEEL AND IN EUROPEAN IT IS USED FOR ITS EXCELLENT CHARACTERISTICS THAT MAKE IT SUITABLE FOR SEVERAL APPLICATIONS. IT HAS A MEDIUM-HIGH HARDENABILITY AND A GOOD MACHINABILITY.AFTER CASE-HARDENING AND HARDENING TREATMENTS, THE SURFACE REACHES AN ELEVATED HARDNESS.17NiCrMo6-4 IS USED FOR THE PRODUCTION OF MECHANICAL PARTS, WHICH ARE SUBMITTED TO WEAR (GEARS, CAMSHAFTS, BUSHINGS, PINIONS).IS USED FOR THE PRODUCTION OF MECHANICAL PARTS, WHICH ARE SUBMITTED TO WEAR (GEARS, CAMSHAFTS, BUSHINGS, PINIONS).
- Other Recommended Materials: 20CrNiMo
CORRESPONDENCE TO INTERNATIONAL DESIGNATIONS
| QUALITY | EUROPE | GERMANY | FRANCE | SPAIN | G.B. | USA | |
|---|---|---|---|---|---|---|---|
| EN | DIN | W.n. | AFNOR | UNE | B.S. | AISI/SAE | |
| 17NiCrMoS6-4 | 17NiCrMoS6-4 | 1.6566 | 18NCD6 | 817M17 | 4317 | ||
17NiCrMo6-4 CHEMICAL COMPOSITION % (EN 10084)
| STEEL DESIGNATION | CHEMICAL COMPOSITION | |||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| SYMBOLIC | NUMERIC | C | Si max | Mn | P max | S | Cr | Mo | Ni | B |
| 17NiCrMo6-4 | 1,6566 | 0,14 ÷ 0,20 | 0,40 | 0,60 ÷ 0,90 | 0,025 | ≤ 0,035 | 0,80 ÷ 1,10 | 0,15 ÷ 0,25 | 1,20 ÷ 1,50 | – |
| 17NiCrMoS6-4 | 1,6569 | 0,020 ÷ 0,040 | ||||||||
CONCENTRATION LIMITS OF THE ELEMENTS THAT ARE NOT INDICATED IN THE TABLE CAN BE DEDUCED IN THE EN 10020 REGULATION. IT CAN BE PROVIDED WITH AN ADDITION OF LEAD 0,12-0,35% OR SULPHUR CONTROLLED UP UNTIL 0,40% FOR AN IMPROVED MACHINABILITY.
MECHANICAL CHARACTERISTICS (UNI 7846)
| STEEL QUALITY | BAR’S DIAMETER | TENSILE TESTING | IMPACT STRENGTH KCU min | ||||
|---|---|---|---|---|---|---|---|
| UNIFIED TENSILE STRENGTH R | DEVIATION FROM PROPORTIONALITY Rp 0,2 min | ELONGATION A min | |||||
| mm | N/mm2 | kgf/mm2 | N/mm2 | kgf/mm2 | % | J | |
| 18NiCrMo5 | 11 (30) (63) | 1230÷1520 (980÷1270) (830÷1130) | 125÷155 (100÷130) (85÷115) | 980 (735) (635) | 100 (75) (65) | 8 (9) (10) | 30 (32,5) (35) |
JOMINY HARDENABILITY (EN 10084)
| STEEL DESIGNATION | RANGE LIMITS | HRC HARDNESS MEASURED FROM THE QUENCHED END OF THE TEST TUBE (MM) | |||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| SYMBOLIC | NUMERIC | 1,5 | 3 | 5 | 7 | 9 | 11 | 13 | 15 | 20 | 25 | 30 | 35 | 40 | |
| 17NiCrMo6-4+H | 1.6566+H | max | 47 | 47 | 46 | 45 | 43 | 42 | 41 | 39 | 37 | 35 | 34 | 34 | 33 |
| 17NiCrMoS6-4+H | 1.6569+H | min | 39 | 38 | 36 | 35 | 32 | 30 | 28 | 26 | 24 | 22 | 21 | 20 | 20 |
| 17NiCrMo6-4+HH | 1.6566+HH | max | 47 | 47 | 46 | 45 | 43 | 42 | 41 | 39 | 37 | 35 | 34 | 34 | 33 |
| 17NiCrMoS6-4+HH | 1.6569+HH | min | 42 | 41 | 39 | 38 | 36 | 34 | 32 | 30 | 28 | 26 | 25 | 25 | 24 |
| 17NiCrMo6-4+HL | 1.6566+HL | max | 44 | 44 | 43 | 42 | 39 | 38 | 37 | 35 | 33 | 31 | 30 | 29 | 29 |
| 17NiCrMoS6-4+HL | 1.6569+HL | min | 39 | 38 | 36 | 35 | 32 | 30 | 28 | 26 | 24 | 22 | 21 | 20 | 20 |
USUALLY AVAILABLE EX STOCK
| QUALITY | HEAT TREATMENT | SURFACE | |
|---|---|---|---|
| 17NiCrMo6-4 | Soft-annealed | rolled forged turned drawn / peeled h111 | |
| 17NiCrMo6-4 high machinability | Soft-annealed | rolled peeled | |
| 17NiCrMo6-4+PB | Soft-annealed | rolled drawn / peeled h111 |