C36000 Description

C36000 Free Cutting Brass is a high-performance copper-zinc alloy engineered specifically for superior machinability. Containing 2.5-3.0% lead for enhanced cutting characteristics, this alloy delivers exceptional chip control, extended tool life, and superior surface finishes. With a machinability rating of 100% (industry standard), C36000 enables high-speed production of precision components while maintaining excellent mechanical properties and good corrosion resistance.

Quick Specifications

PropertyValuePropertyValue
Alloy DesignationC36000 (Alloy 360)Machinability Rating100% (Standard)
Copper Content60.0-63.0%Lead Content2.5-3.0%
Tensile Strength338-485 MPaElectrical Conductivity26% IACS
Thermal Conductivity115 W/m·KDensity8.49 g/cm³

Category:

C36000 Free Cutting Brass – Technical Product Introduction

Product Overview

C36000 Free Cutting Brass, also known as Alloy 360 or Free Machining Brass, is a copper-zinc alloy specifically engineered for exceptional machinability. This alloy incorporates controlled amounts of lead to significantly enhance cutting characteristics, making it the industry standard for high-speed machining operations and precision component manufacturing.

Key Technical Features

FeatureSpecificationTechnical Advantage
Machinability Rating100% (industry standard)Fastest cutting speeds, best chip control
Lead Content2.5-3.0%Optimal chip breaking and tool lubrication
Surface Finish CapabilityRa 0.4-0.8 μmMinimal secondary finishing required
Thermal Conductivity115 W/m·KExcellent heat dissipation during machining
Electrical Conductivity26% IACSSuitable for electrical applications
Corrosion ResistanceGood in atmospheric conditionsLong-term durability in most environments

Chemical Composition

Standard Chemical Composition (ASTM B16)

ElementContent (%)FunctionTypical Analysis
Copper (Cu)60.0-63.0Base metal for strength and conductivity61.5
Zinc (Zn)RemainderStrength enhancement and cost optimization35.5
Lead (Pb)2.5-3.0Machinability enhancement and chip control2.8
Iron (Fe)≤0.35Controlled impurity0.15
Nickel (Ni)≤0.5Minor alloying element0.25
Aluminum (Al)≤0.05Deoxidizer0.02
Other Elements≤0.5 totalControlled impurities–

Compositional Comparison with Related Alloys

AlloyCu (%)Zn (%)Pb (%)Primary Characteristic
C3600060.0-63.0Rem2.5-3.0Excellent machinability
C2600068.5-71.5Rem–High ductility
C3850056.0-59.0Rem2.5-3.5Architectural applications
C4640059.0-62.0Rem–Naval brass
C3530060.0-63.0Rem1.5-2.5Medium lead content

Mechanical Properties

Mechanical Properties by Temper Condition

Temper DesignationTensile Strength (MPa)Yield Strength (MPa)Elongation (%)Hardness (Rb)Reduction of Area (%)
O61 (Annealed)338-380124-14045-5350-6055-65
H01 (1/4 Hard)370-415140-31025-3562-7545-55
H02 (1/2 Hard)415-450165-34520-3075-8535-45
H04 (Full Hard)450-485180-38015-2580-9025-35

Fatigue and Impact Properties

PropertyValueTest ConditionStandard
Fatigue Strength140-160 MPa10⁸ cycles, rotating beamASTM D7791
Impact Strength35-45 JCharpy V-notch, room temperatureASTM E23
Fracture Toughness45-55 MPa√mPlane strain conditionsASTM E399
Endurance Limit130-150 MPaFully reversed loadingASTM D7791

Physical Properties

Thermal and Electrical Properties

PropertyValueUnitTemperature (°C)Test Method
Density8.49g/cm³20ASTM B311
Melting Point (Solidus)885°C–DSC Analysis
Melting Point (Liquidus)900°C–DSC Analysis
Thermal Conductivity115W/m·K20ASTM E1461
Thermal Conductivity125W/m·K100ASTM E1461
Electrical Conductivity26% IACS20ASTM B193
Electrical Resistivity0.066μΩ·m20ASTM B193

Thermal Expansion and Modulus Properties

PropertyValueUnitTemperature RangeStandard
Coefficient of Linear Expansion20.5μm/m·°C20-100°CASTM E831
Coefficient of Linear Expansion21.0μm/m·°C20-200°CASTM E831
Modulus of Elasticity97GPa20°CASTM E111
Shear Modulus37GPa20°CASTM E143
Poisson’s Ratio0.34–20°CASTM E132
Specific Heat Capacity377J/kg·K20°CASTM E1269

Machinability Characteristics

Optimal Machining Parameters

OperationSpeed (m/min)Feed Rate (mm/rev)Depth of Cut (mm)Tool GeometrySurface Finish (Ra μm)
Turning – Roughing150-3000.25-0.502.0-5.0CNMG, DNMG1.6-3.2
Turning – Finishing200-4000.05-0.200.5-2.0CNMG, VCMT0.4-0.8
Face Milling100-2000.10-0.301.0-3.0Face mill insert0.8-1.6
End Milling80-1500.08-0.201.0-2.0Carbide end mill0.8-1.6
Drilling (HSS)30-600.10-0.30–118° point angle1.6-3.2
Drilling (Carbide)60-1200.15-0.35–130° point angle1.6-3.2
Reaming15-300.20-0.500.1-0.3Straight flute0.4-0.8
Threading20-40Pitch dependent–60° threading tool1.6-3.2

Tool Life and Machining Performance

Cutting Tool MaterialRelative Tool LifeRecommended ApplicationCutting Speed Range
High-Speed Steel (HSS)100% (baseline)General machining, drilling, tapping30-100 m/min
Uncoated Carbide200-300%High-speed turning, milling100-300 m/min
TiN Coated Carbide300-400%Extended tool life applications150-400 m/min
TiAlN Coated Carbide350-450%High-speed finishing200-500 m/min
CBN (Cubic Boron Nitride)500-800%Ultra-high-speed machining300-800 m/min

Chip Formation and Control

Machining OperationChip TypeChip Control RatingRecommended BreakTool Wear Pattern
TurningShort, broken chipsExcellentChip breaker geometryUniform flank wear
MillingSmall segmentsVery goodPositive rake angleCorner wear
DrillingRibbon chipsGoodProper point geometryFlank wear on margins
ThreadingFine chipsExcellentSharp cutting edgeMinimal wear

Applications and Uses

Primary Application Categories

Industry SectorComponent ExamplesPerformance RequirementsMaterial Benefits
AutomotiveFuel system fittings, brake line fittings, electrical terminalsPrecision, pressure resistance, corrosion resistanceEasy machining, tight tolerances achievable
Electrical/ElectronicsConnectors, terminals, switch components, grounding screwsElectrical conductivity, precision, reliabilityGood conductivity, excellent machinability
Plumbing/HVACPipe fittings, valve components, compression fittingsPressure rating, corrosion resistance, reliabilityCost-effective, good sealing properties
Industrial MachineryGears, bushings, bearings, mechanical fastenersWear resistance, dimensional stability, strengthSelf-lubricating lead content
Marine HardwareNon-critical fasteners, decorative hardwareCorrosion resistance in freshwater environmentsGood atmospheric corrosion resistance
Musical InstrumentsValve assemblies, slides, mechanical componentsSmooth operation, precision, durabilityExcellent surface finish capability

Specific Component Applications

Component TypeTypical Size RangeCritical RequirementsManufacturing Process
NPT Threaded Fittings1/8″ to 4″ pipe sizeThread accuracy, pressure sealingCNC turning, thread cutting
Electrical Terminals2mm to 50mm widthConductivity, crimp retentionStamping, CNC machining
Valve Bodies1/4″ to 6″ port sizePressure rating, leak-proofCNC machining, drilling
Gear Components10mm to 300mm diameterTooth accuracy, wear resistanceGear cutting, heat treatment
Bushings/Bearings5mm to 150mm boreDimensional accuracy, surface finishTurning, boring, reaming
Custom ConnectorsApplication specificElectrical properties, fit tolerancesMulti-axis CNC machining

Performance in Service Environments

EnvironmentCorrosion ResistanceTemperature LimitSuitability RatingLimitations
Indoor AtmosphericExcellent-40°C to +200°CExcellentNone significant
Outdoor AtmosphericGood-40°C to +150°CGoodRegular maintenance recommended
Fresh WaterGood0°C to +80°CGoodAvoid stagnant conditions
Marine (Seawater)PoorN/ANot recommendedUse naval brass instead
Industrial ChemicalsVariableDepends on chemicalCase-by-case evaluationChemical compatibility testing required
High TemperatureGoodUp to 200°C continuousGoodOxidation resistance acceptable

Available Product Forms

Standard Product Forms and Dimensions

Product FormSize RangeStandard LengthsTolerance ClassSurface Condition
Round Bar3mm – 350mm diameter1m, 2m, 3m, 4m, 6mh9, h11 (ISO 286)Bright drawn, centerless ground
Hexagonal Bar5mm – 150mm across flats1m, 2m, 3m, 4m±0.13mmBright drawn
Square Bar5mm – 100mm square1m, 2m, 3m, 4m±0.13mmBright drawn
Rectangular Bar3-60mm × 10-200mm1m, 2m, 3m, 4m±0.15mmCold drawn, mill finish
Hollow Bar (Tube)10-300mm OD, 2-250mm wall1m, 2m, 3m, 6m±0.20mmAs drawn, bright
Wire0.5mm – 15mm diameterCoils or cut lengths±0.05mmBright drawn

Dimensional Tolerances and Surface Finish

Diameter Range (mm)Standard Tolerance (mm)Precision Tolerance (mm)Surface Roughness (Ra μm)Straightness Tolerance
3-6±0.05±0.020.4-0.80.5mm/m
6-10±0.08±0.030.4-0.80.5mm/m
10-18±0.10±0.040.6-1.00.3mm/m
18-30±0.13±0.050.8-1.20.3mm/m
30-50±0.16±0.060.8-1.60.2mm/m
50-80±0.19±0.081.0-1.60.2mm/m
80-120±0.22±0.101.2-2.00.15mm/m
120-200±0.25±0.121.6-2.50.15mm/m

Standards and Specifications

International Standards Compliance

StandardFull DesignationGeographic ScopeSpecification Coverage
ASTM B16/B16MFree-Cutting Brass Rod, Bar and ShapesNorth AmericaChemical composition, mechanical properties, dimensions
EN 12164Copper and copper alloys – Rod for machining purposesEuropeManufacturing requirements, tolerances, testing
JIS H3250Copper and copper alloy rods and barsJapanChemical composition, mechanical properties, inspection
ISO 426-2Wrought copper-zinc alloys – Chemical composition and formsInternationalDesignation system, chemical limits
BS EN 12163Copper and copper alloys – Rod for general purposesUnited KingdomGeneral specifications, quality requirements
DIN 17660Copper-zinc alloys – Chemical composition and mechanical propertiesGermanyMaterial specifications, testing methods

Chemical Composition Limits by Standard

StandardCu (%)Zn (%)Pb (%)Fe (%)Other Elements
ASTM B1660.0-63.0Remainder2.5-3.0≤0.35Ni ≤0.5%, others ≤0.5% total
EN 1216460.0-63.0Remainder2.5-3.0≤0.35Ni ≤0.5%, Al ≤0.05%
JIS H325060.0-63.0Remainder2.5-3.0≤0.35Similar to ASTM
ISO 426-260.0-63.0Remainder2.5-3.0≤0.35Harmonized with EN

Mechanical Property Requirements by Standard

StandardTensile Strength (MPa)Yield Strength (MPa)Elongation (%)Hardness
ASTM B16 (O61)338-380124 min15 min50-70 Rb
ASTM B16 (H02)415-485275 min8 min75-90 Rb
EN 12164 (M)340-430140 min15 min60-85 HB
JIS H3250 (O)340-390130 min15 min60-80 HB

Heat Treatment and Processing

Heat Treatment Specifications

Treatment TypeTemperature Range (°C)Time at TemperatureCooling MethodResulting Properties
Annealing (O61)425-6501-4 hoursAir coolSoft, maximum ductility
Stress Relief200-3001-2 hoursAir coolReduced internal stress
Solution Treatment700-7501 hourWater quenchHomogeneous structure
Process Annealing300-40030-60 minutesAir coolPartial softening

Processing Characteristics

ProcessFormability RatingTemperature RequirementsSpecial Considerations
Cold WorkingGoodRoom temperatureWork hardening occurs, periodic annealing may be needed
Hot WorkingExcellent600-750°CBest formability, avoid overheating
WeldingFairVariousLead vaporization concern, ventilation required
BrazingGood600-850°CCompatible with most brazing alloys
SolderingExcellent180-250°CEasy to solder, good joint strength

Quality Control and Testing

Standard Test Methods

PropertyTest MethodSample SizeFrequencyAcceptance Criteria
Chemical CompositionXRF Spectroscopy (ASTM E1086)3 pieces per heatEvery heatWithin specification limits
Tensile PropertiesTensile Test (ASTM E8)2 specimens per lotPer production lotMeet standard requirements
HardnessRockwell B (ASTM E18)3 readings per pieceStatistical samplingWithin specified range
Dimensional AccuracyCoordinate Measuring (ASTM E1)100% or samplingContinuousWithin tolerance
Surface QualityVisual Inspection (ASTM B250)100%ContinuousNo defects
MicrostructureMetallography (ASTM E3)1 per production runWeeklyUniform α+β structure

Defect Classification and Limits

Defect TypeClass A (Critical)Class B (Major)Class C (Minor)Detection Method
Chemical CompositionOut of specificationNear limits–Spectroscopic analysis
Dimensional Variation>2× tolerance>1.5× tolerance>toleranceDimensional measurement
Surface DefectsCracks, deep scratchesShallow scratchesLight marksVisual inspection
Hardness Deviation>±10 points>±5 pointsWithin ±5 pointsHardness testing
Internal DefectsVoids, inclusionsMinor porosity–Ultrasonic testing

Environmental and Safety Considerations

Material Safety Information

Hazard CategoryRisk LevelPrimary ConcernSafety Measures
Lead ContentModerateIngestion, inhalation of dust/fumesUse ventilation, avoid machining dust inhalation
Machining OperationsLowMetal dust generationStandard machine shop practices
Welding/BrazingModerateLead fume generationAdequate ventilation, respiratory protection
Fire HazardVery LowNon-combustible metalStandard fire precautions
EnvironmentalModerateLead content requires proper disposalFollow local regulations for metal waste

Recycling and Disposal

AspectRequirementCompliance Method
Material IdentificationLead content declarationMaterial certification documentation
Scrap SegregationSeparate leaded brass collectionDesignated scrap containers
Recycling ProcessSpecialized brass recyclingCertified metal recyclers
Waste DisposalHazardous waste classificationLicensed waste disposal services
DocumentationChain of custody recordsMaterial tracking systems

This technical specification provides comprehensive information about C36000 Free Cutting Brass for engineering and manufacturing applications.