C24000 PRODUCT DESCRIPTION:
Low Brass 80%
TEMPERS: H01 Quarter Hard, H02 Half Hard, H04 Hard
SOLIDS: 3/8″ to 2 1/2″ O.D.
HEX: 3/8″ to 2″ O.D.
STANDARD LENGTHS: 144″
C24000 Typical Uses
ARCHITECTURE: medallions, ornamental components, spandrels
BUILDERS HARDWARE: decorative panels
CONSUMER: clock dials, musical instrument parts, plaques
ELECTRICAL: battery caps, rotor bars (AC motors)
INDUSTRIAL: flexible hose, flexible hose bellows, pump lines, welding wire
OTHER tokens
C24000 Typical Uses
ARCHITECTURE: medallions, ornamental components, spandrels
BUILDERS HARDWARE: decorative panels
CONSUMER: clock dials, musical instrument parts, plaques
ELECTRICAL: battery caps, rotor bars (AC motors)
INDUSTRIAL: flexible hose, flexible hose bellows, pump lines, welding wire
OTHER tokens
C24000 brass extruded rod is a high-quality brass product commonly used to manufacture a variety of parts and structural parts that require high strength and corrosion resistance. This brass rod is manufactured using an extrusion process, so it has better mechanical properties and processing properties.
The main components of C24000 brass extruded rod are copper and zinc, of which the copper content is relatively high, usually above 60%. This kind of brass has high strength, hardness, corrosion resistance and wear resistance, and can be used in a variety of different environments and conditions. In addition, C24000 brass extruded rods also have good electrical and thermal conductivity and can be used to manufacture parts and structural parts that need to transmit current or heat.
During the manufacturing process, C24000 brass extruded rods require multiple passes of extrusion and annealing to obtain the required mechanical properties and processing properties. In addition, in order to improve the corrosion resistance and wear resistance of brass rods, some alloying elements, such as iron, nickel, etc., can be added during the manufacturing process. The addition of these alloying elements can change the microstructure and properties of brass, making it more suitable for different use needs.
C24000 brass extruded rods have a wide range of applications and can be used to manufacture a variety of parts and structural parts that require high strength and corrosion resistance, such as bolts, nuts, bushings, gears, etc. In addition, due to its good electrical and thermal conductivity, C24000 brass extruded rods can also be used to manufacture wires and cables, electronic components, radiators and other products.
In short, C24000 brass extruded rod is a high-quality brass product with excellent mechanical properties, processing performance, corrosion resistance and wear resistance. Its wide range of applications makes it play an important role in various fields.
C24000 Similar or Equivalent Specification
| CDA | ASTM | SAE | AMS | Federal | Military | Other |
|---|---|---|---|---|---|---|
| C24000 | B927 B927M |
C24000 Chemical Composition
| Cu% | Pb% | Zn% | Fe% | ||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
Chemical Composition according to ASTM B927/B927M-17 Note: Cu + Sum of Named Elements, 99.8% min. Single values represent maximums. | |||||||||||
| 78.50- 81.50 | 0.05 | Rem. | 0.05 | ||||||||
C24000 Machinability
| Copper Alloy UNS No. | Machinability Rating | Density (lb/in3 at 68 °F) |
|---|---|---|
| C24000 | 30 | 0.313 |
C24000 Mechanical Properties
C24000
H01 Quarter Hard
SIZE RANGE: UNDER 1/2″ DIAMETER ROD
| Tensile Strength, min | Yield Strength, at 0.5% Extension Under Load, min | Elongation, 4x Diameter or 4x Thickness, min | Rockwell “B” Hardness | Remarks | ||
|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | % | typical HRB | |
| 47 | 325 | 25 | 170 | 18 | 55 | |
SIZE RANGE: OVER 1/2″ DIAMETER ROD TO 1″ INCLUSIVE
| Tensile Strength, min | Yield Strength, at 0.5% Extension Under Load, min | Elongation, 4x Diameter or 4x Thickness, min | Rockwell “B” Hardness | Remarks | ||
|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | % | typical HRB | |
| 45 | 310 | 20 | 140 | 20 | 55 | |
SIZE RANGE: OVER 1″ DIAMETER ROD
| Tensile Strength, min | Yield Strength, at 0.5% Extension Under Load, min | Elongation, 4x Diameter or 4x Thickness, min | Rockwell “B” Hardness | Remarks | ||
|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | % | typical HRB | |
| 43 | 295 | 18 | 125 | 22 | 55 | |
C24000
H02 Half Hard
SIZE RANGE: UNDER 1/2″ DIAMETER ROD
| Tensile Strength, min | Yield Strength, at 0.5% Extension Under Load, min | Elongation, 4x Diameter or 4x Thickness, min | Rockwell “B” Hardness | Remarks | ||
|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | % | typical HRB | |
| 53 | 365 | 33 | 230 | 10 | 70 | |
SIZE RANGE: OVER 1/2″ DIAMETER ROD TO 1″ INCLUSIVE
| Tensile Strength, min | Yield Strength, at 0.5% Extension Under Load, min | Elongation, 4x Diameter or 4x Thickness, min | Rockwell “B” Hardness | Remarks | ||
|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | % | typical HRB | |
| 48 | 330 | 30 | 205 | 13 | 70 | |
SIZE RANGE: OVER 1″ DIAMETER ROD
| Tensile Strength, min | Yield Strength, at 0.5% Extension Under Load, min | Elongation, 4x Diameter or 4x Thickness, min | Rockwell “B” Hardness | Remarks | ||
|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | % | typical HRB | |
| 43 | 295 | 28 | 195 | 15 | 70 | |
C24000
H04 Hard
SIZE RANGE: UNDER 1/2″ DIAMETER ROD
| Tensile Strength, min | Yield Strength, at 0.5% Extension Under Load, min | Elongation, 4x Diameter or 4x Thickness, min | Rockwell “B” Hardness | Remarks | ||
|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | % | typical HRB | |
| 68 | 470 | 45 | 310 | 8 | 82 | |
SIZE RANGE: OVER 1/2″ DIAMETER ROD TO 1″ INCLUSIVE
| Tensile Strength, min | Yield Strength, at 0.5% Extension Under Load, min | Elongation, 4x Diameter or 4x Thickness, min | Rockwell “B” Hardness | Remarks | ||
|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | % | typical HRB | |
| 65 | 450 | 40 | 275 | 10 | 82 | |
SIZE RANGE: OVER 1″ DIAMETER ROD
| Tensile Strength, min | Yield Strength, at 0.5% Extension Under Load, min | Elongation, 4x Diameter or 4x Thickness, min | Rockwell “B” Hardness | Remarks | ||
|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | % | typical HRB | |
| 60 | 415 | 35 | 240 | 12 | 82 | |
C24000 Physical Properties
Physical Properties provided by CDA | |||||||||||
| US Customary | Metric | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Melting Point – Liquidus | 1830 °F | 999 °C | |||||||||
| Melting Point – Solidus | 1770 °F | 966 °C | |||||||||
| Density | 0.313 lb/in3 at 68 °F | 8.67 gm/cm3 at 20 °C | |||||||||
| Specific Gravity | 8.67 | 8.67 | |||||||||
| Electrical Conductivity | 32% IACS at 68 °F | 0.186 MegaSiemens/cm at 20 °C | |||||||||
| Thermal Conductivity | 81 Btu/sq ft/ft hr/°F at 68 °F | 140.3 W/m at 20 °C | |||||||||
| Coefficient of Thermal Expansion 68-572 | 10.6 · 10-6 per °F (68-572 °F) | 18.4 · 10-6 per °C (20-300 °C) | |||||||||
| Specific Heat Capacity | 0.09 Btu/lb/°F at 68 °F | 377.1 J/kg at 20 °C | |||||||||
| Modulus of Elasticity in Tension | 16000 ksi | 110317 MPa | |||||||||
| Modulus of Rigidity | 6000 ksi | 41369 MPa | |||||||||
C24000 Fabrication Properties
Fabrication Properties provided by CDA | |||||||||||
| Technique | Suitability | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Soldering | Excellent | ||||||||||
| Brazing | Excellent | ||||||||||
| Oxyacetylene Welding | Good | ||||||||||
| Gas Shielded Arc Welding | Good | ||||||||||
| Coated Metal Arc Welding | Not Recommended | ||||||||||
| Spot Weld | Fair | ||||||||||
| Seam Weld | Not Recommended | ||||||||||
| Butt Weld | Good | ||||||||||
| Capacity for Being Cold Worked | Excellent | ||||||||||
| Capacity for Being Hot Formed | Fair | ||||||||||
| Machinability Rating | 30 | ||||||||||
C24000 Thermal Properties
Thermal Properties provided by CDA *Temperature is measured in Fahrenheit. | |||||||||||
| Treatment | Minimum* | Maximum* | |||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Annealing | 800 | 1300 | |||||||||
| Hot Treatment | 1500 | 1650 | |||||||||
C24000 Common Fabrication Processes
Blanking, Drawing, Etching, Forming and Bending, Heading and Upsetting, Piercing and Punching, Roll Threading and Knurling, Shearing, Spinning, Squeezing and Swaging, Stamping
Common Fabrication Processes provided by CDA