C95800 Nickel Aluminum Bronze (NAB) Marine Grade Alloy

C95800 (Alpha NAB) is the premier alloy for extreme seawater and high-load industrial applications. It combines the strength of steel with the unmatched corrosion resistance of nickel-bronze.
FeatureTechnical Benefit
Corrosion ResistanceSelf-healing Al2O3 film prevents pitting and dealuminization
High StrengthTensile 585 MPa min; superior fatigue and impact resistance
Cavitation DefenseOutperforms 316 Stainless Steel in high-velocity flows
Anti-BiofoulingNatural copper content inhibits barnacle and algae growth
Non-MagneticPermeability less than 1.05; ideal for naval and sonar use

Key Specifications:

  • Standards: ASTM B148/B505 (C95800), EN 1982 (CC333G), BS 1400 (AB2)
  • Applications: Propellers, sea valves, pump impellers, and heavy-duty bushings
  • Quality: Certified to EN 10204 3.1 with NDT testing (UT/PT) available
Available in: Sand/Centrifugal Castings, Continuous Bars, and Custom CNC Machined Parts.

Category:

C95800 Overview

C95800 (Nickel Aluminum Bronze) is a premium casting alloy specifically designed to withstand the harshest corrosive environments. By incorporating 4-5% Nickel and 4% Iron, the alloy develops a stabilized microstructure that prevents dealuminization. Its self-healing aluminum oxide surface film makes it nearly immune to pitting and crevice corrosion in aerated seawater.

Technical Specifications

Chemical Composition (ASTM B148)

ElementSymbolComposition (%)
CopperCu79.0 min
AluminumAl8.5 – 9.5
NickelNi4.0 – 5.0
IronFe3.5 – 4.5
ManganeseMn0.8 – 1.5
SiliconSi0.10 max
LeadPb0.03 max

Mechanical Properties (Minimum Requirements)

PropertyValue (Metric)Value (Imperial)
Tensile Strength (Min)585 MPa85,000 psi
Yield Strength (Min)240 MPa35,000 psi
Elongation (in 2″)15%15%
Brinell Hardness150 – 190 HBW150 – 190 HBW
Machinability Rating20%(Relative to C360)

Physical Properties

  • Density: 7.64 g/cm³ (0.276 lb/in³)
  • Thermal Conductivity: 36 W/m·K
  • Electrical Conductivity: 7% IACS
  • Magnetic Permeability: < 1.05 (Ideal for non-magnetic naval applications)

Advanced Features

  • Cavitation & Erosion Resistance: C95800 outperforms most stainless steels in high-speed fluid flow, making it essential for pump and turbine components.
  • Biofouling Resistance: The high copper content naturally inhibits the growth of barnacles and algae, reducing maintenance costs for underwater hardware.
  • Weldability: Excellent rating. Can be easily repaired or joined using MIG/TIG welding with ERCuNiAl filler metal.
  • Temper Annealing: Our products undergo professional stabilization (6-hour soak at 650°C) to ensure the highest level of corrosion resistance post-casting.

Global Cross-Reference Table

We supply C95800 manufactured to meet various international standards:

  • USA: ASTM B148 / B505 C95800
  • Europe: EN 1982 CC333G (CuAl10Fe5Ni5-C)
  • UK: BS 1400 AB2
  • Japan: JIS H5121 CAC703 (AlBC3)
  • Germany: DIN 1714 G-CuAl10Ni

Typical Applications

  • Maritime: Ship propellers, hubs, stern tube bearings, sea water intake screens.
  • Energy: Desalination plant components, brine heaters, offshore firewater pumps.
  • Industrial: Worm gears, heavy-duty bushings, high-pressure valve bodies.

Order & Customization: We provide C95800 in sand cast, centrifugal cast, and continuous cast forms. Contact our sales engineering team for custom dimensions, NDT testing (UT/PT/RT), or material certification (EN 10204 3.1).