Qsn8-0.3 Description
Qsn8-0.3 tin bronze is bronze with tin as the main alloying element. Tin content in general between 3 ~ 14%, mainly used for making elastic components and wear-resistant parts.
Chemical Component
Sn:7.0-9.0
P:0.03-0.35
Zn:≤0.20
Ni:≤0.20
Fe:≤0.01
Pb:≤0.05
Cu:Remain
Mechanical Properties
Tensile strength σ B (MPa) : ≥350
Elongation δ10 (%) : ≥55
Note: Longitudinal tensile mechanical properties of bar at room temperature
Sample size: diameter or opposite side distance 40 ~ 120
Qsn8-0.3 tin bronze is bronze with tin as the main alloying element. Tin content in general between 3 ~ 14%, mainly used for making elastic components and wear-resistant parts.
| 
 | |
| Lion standard | QSn8-0.3 | 
| QSn8-0.3 | |
| American standard | C52100 | 
| Japanese standard | C5210 | 
| Chemical composition (weight percent) | |
| Sn | 7.0-9.0 | 
| P | 0.03-0.35 | 
| With | margin | 
| Sum of impurities | ≤ 0.5 | 
| Physical properties (room temperature) | ||
| Conductivity | ≥ 12 | %IACS | 
| Conductivity | ≥ 6.96 | MS/m | 
| Thermal conductivity | 62 | W/(m.K) | 
| Thermal expansion coefficient | 18.2 | 10 -6 / K | 
| Density | 8.8 | g/cm3 | 
| Elastic Modulus | 110 | GPa | 
| Specific heat capacity | 380 | J/(g.K) | 
| Poisson’s ratio | 0.33 | — | 
| Process performance | |
| Cold workability | Excellent | 
| Machinability | Generally | 
| Electroplating | Good | 
| Hot-dip tinning | Good | 
| Solderability | Excellent | 
| Resistance welding | Good | 
Typical use
| Mechanical behavior | ||||
| State | Tensile Strength ( MPa ) | Elongation ( A 11.3 , % ) | Vickers hardness | |
| M | O60 | ≥ 345 | ≥ 45 | ≤ 120 | 
| Y 4 | H01 | 390-510 | ≥ 40 | 100-160 | 
| Y 2 | H02 | 490-610 | ≥ 30 | 150-205 | 
| AND | H04 | 590-705 | ≥ 12 | 180-235 | 
| T | H06 | 680-740 | ≥ 5 | 200-250 | 
| TY | H08 | 735-833 | ≥ 2 | 230-270 | 
Mainly used in the manufacture of elastic components, wear-resistant parts and anti-magnetic parts in precision instruments, such as spring contact pieces or other springs with good electrical conductivity; various altimeters in the aviation industry, springs for lifting speedometers, connecting rods, etc. , Gears, brush boxes, contactors, etc. in precision instruments.
| Thickness tolerance | ||||||
| Thickness ( mm ) | 0.08-0.15 | >0.15-0.20 | >0.2-0.3 | >0.3-0.4 | >0.4-0.6 | >0.6-0.8 | 
| Tolerance ( mm ) | ± 0.0025 | ± 0.004 | ± 0.005 | ± 0.0075 | ± 0.01 | ± 0.0125 | 
| Thickness ( mm ) | >0.8-1.2 | >1.2-1.5 | >1.5-2.0 | >2.0-2.6 | >2.6-3.0 | >3.0-4.0 | 
| Tolerance ( mm ) | ± 0.015 | ± 0.02 | ± 0.025 | ± 0.03 | ± 0.04 | ± 0.05 | 
| Width tolerance | ||||||
| Thickness ( mm ) | 0.08-0.5 | >0.5-1.0 | >1.0-1.8 | >1.8-3.0 | >3.0-4.0 | |
| Width and Tolerance (mm) | 5-50 | ± 0.05 | ± 0.08 | ± 0.1 | ± 0.2 | ± 0.3 | 
| >50-100 | ± 0.075 | ± 0.1 | ± 0.15 | ± 0.2 | ± 0.3 | |
| >100 | ± 0.1 | ± 0.15 | ± 0.2 | ± 0.3 | ± 0.5 | 
| Glitch | |
| Thickness ( mm ) | Edge Burr ( mm ), no greater than | 
| ≤ 0.50 | 0.02 | 
| >0.50-1.0 | 0.04 | 
| >1.0-2.0 | 0.05 | 
| >2.0-4.0 | 0.1 | 
| Bending performance | ||||
| Condition | Minimum Bend Inside Radius ( mm ) | |||
| Thickness /t : 0.15-0.30mm | Thickness /t : 0.30-1.0mm | |||
| Good direction | Bad direction | Good direction | bad direction | |
| O60 | 0 × t | 0 × t | 0 × t | 0 × t | 
| H01 | 0 × t | 0 × t | 0 × t | 0 × t | 
| H02 | 0 × t | 0 × t | 0 × t | 0 × t | 
| H04 | 0 × t | 1.0 × t | 1.0 × t | 2.0 × t | 
| H06 | 1.5 × t | 4.0 × t | 2.0 × t | 5.0 × t | 
| H08 | – | – | – | – | 
| Surface roughness | |
| Ra (μ m ) | ≤ 0.3 | 
| Side curvature h ( mm/m ) | |||
| Width ( mm ) | Thickness ( mm ) | ||
| 0.08-0.6 | >0.6-2.0 | 2.0-4.0 | |
| ≤ 9 | ≤ 1.0 | ≤ 1.0 | — | 
| >9-13 | ≤ 1.0 | ≤ 1.0 | — | 
| >13-25 | ≤ 1.0 | ≤ 1.0 | — | 
| >25-50 | ≤ 1.5 | ≤ 1.0 | — | 
| >50-100 | ≤ 1.5 | ≤ 1.5 | — | 
| >100-625 | ≤ 1.5 | ≤ 1.5 | — | 
| Lateral curvature | |||
| Width L ( mm ) | ≤ 50 | >50-200 | >200-625 | 
| Transverse curvature h ( mm ), not more than | 0.01 × L | 0.015 × L | 0.02 × L | 
| Longitudinal flatness (serpentine) | ||
| Width ( mm ) | ≤ 100 | >100-625 | 
| Longitudinal straightness h ( mm/m ) | ≤ 3 | ≤ 5 | 
| Twist | |||
| Width ( mm ) | ≤ 30 | >30-100 | >100-625 | 
| Torsion (°) | ≤ 10 | ≤ 5 | — | 
| Warpage | |||
| Width ( mm ) | ≤ 100 | >100-300 | >300-625 | 
| Warpage h ( mm/m ) | ≤ 50 | ≤ 100 | — | 
 