QSn4-0.3 Tin bronze

Grade: QSn4-0.3

Standard: GB/T 4423-1992

Features and scope of application:

Qsn4-0.3 tin bronze has high mechanical properties, corrosion resistance and high elasticity. It can withstand pressure machining well in cold state and can also be processed under pressure in hot state. Qsn4-0.3 is used to make all kinds of pressure gauge tube

Category: Tag:
QSn4-0.3 has high mechanical properties, corrosion resistance and elasticity, can bear pressure processing in cold state, also can carry out pressure processing in hot state.

QSn4-0.3 Alloy grade

Lion standardQsn4-0.3
China standardQSn4-0.3
American standardC51100
Japanese standardC5101

QSn4-0.3 Chemical composition (weight percent)

Sn
3.5-4.9
P
0.03-0.35
With
margin
Sum of impurities
≤ 0.95

QSn4-0.3 Physical properties (room temperature)

≥ 16
%IACS
Conductivity
≥ 9.28
MS/m
Thermal conductivity
84
W/(m.K)
Thermal expansion coefficient
17.8
10 -6 / K
Density
8.86
g/cm3
Elastic Modulus
110
GPa
specific heat capacity
0.380 _
J/(g.K)
Poisson’s ratio
0.33
—

QSn4-0.3 Process performance

Cold workability
Excellent
Machinability
Generally
Electroplating
Excellent
Hot-dip tinning
Excellent
Solderability
Excellent
Resistance welding
Generally

Typical use

Widely used in bridge support plates, clutch friction plates, connectors , diaphragms, fuse clips, fasteners, lock washers, springs, switch parts, terminals, chemical equipment components, porous sheets, textile machinery, etc.

Mechanical behavior

State
Tensile Strength ( MPa )
Elongation ( A 11.3 , % )
Vickers hardness
M
O60
275-380
≥ 40
70-100
Y2
H02
380-485
15
90-165
AND
H04
495-600
8
145-190
T
H06
580-685
3
170-210
TY
H08
625-725
–
180-220
CTY
H10
660-750
–
190-240

Thickness tolerance

Thickness ( mm )
0.08-0.15
>0.15-0.20
>0.20-0.30
>0.3-0.4
>0.4-0.6
>0.6-0.8
Tolerance ( mm )
± 0.0025
± 0.004
± 0.005
± 0.0075
± 0.01
± 0.0125
Thickness ( mm )
>0.8-1.2
>1.2-1.5
>1.5-2.0
>2.0-2.6
>2.6-3.0
>3.0-4.0
Tolerance ( mm )
± 0.015
± 0.02
± 0.025
± 0.03
± 0.04
± 0.05

Width tolerance

Thickness ( mm )
0.08-0.5
>0.5-1.0
>1.0-1.8
>1.8-3.0
>3.0-4.0
Width and Tolerance
(mm)
5-50
± 0.05
± 0.08
± 0.1
± 0.2
± 0.3
50-100
± 0.075
± 0.1
± 0.15
± 0.2
± 0.3
> 100
± 0.1
± 0.15
± 0.2
± 0.3
± 0.5

Glitch

Thickness ( mm )
Edge Burr ( mm ), no greater than
≤ 0.50
0.02
>0.50-1.0
0.04
>1.0-2.0
0.05
>2.0-4.0
0.1

QSn4-0.3

Bending performance

condition
Minimum Bend Inside Radius ( mm )
Thickness /t : 0.15-0.30mm
Thickness /t : 0.30-1.0mm
good direction
bad direction
good direction
bad direction
O60
0 × t
0 × t
0 × t
0 × t
H02
0 × t
0 × t
0 × t
0 × t
H04
0 × t
0 × t
0 × t
0.5 × t
H06
1.0 × t
4.0 × t
1.5 × t
5.0 × t
H08
–
–
–
–
H10
–
–
–
–

Surface roughness

Ra (μ m )
≤ 0.3
Side curvature h ( mm/m )
Width ( mm )
Thickness ( mm )
0.08-0.6
>0.6-2.0
>2.0-4.0
≤ 9
≤ 1.0
≤ 1.0
—
>9-13
≤ 1.0
≤ 1.0
—
>13-25
≤ 1.0
≤ 1.0
—
>25-50
≤ 1.5
≤ 1.0
—
>50-100
≤ 1.5
≤ 1.5
—
>100-625
≤ 1.5
≤ 1.5
—

Lateral curvature

Width L ( mm )
≤ 50
>50-200
>200-625
Transverse curvature h ( mm ), not more than
0.01 × L
0.015 × L
0.02 × L
Longitudinal flatness (serpentine)
Width ( mm )
≤ 100
>100-625
Longitudinal straightness h ( mm/m )
≤ 3
≤ 5

Twist

Width ( mm )
≤ 30
>30-100
>100-625
Torsion (°)
≤ 10
≤ 5
—

 

Warpage

Width ( mm )
≤ 100
>100-300
>300-625
Warpage h ( mm/m )
≤ 50
≤ 100
—