Although aluminum alloy 6082 and 6061 belong to 6 series of alloys (silicon and magnesium alloy), they are still different. The main difference is that 6082 and 6061 have different proportions of silicon and magnesium. 1, aluminum alloy 6061: Si is 0.4-0.8, Mg is 0.8-1.2, Fe is 0.7. The main alloying elements of 6061 aluminum...