What is copper alloy strip?

Copper alloy coil strip is a strip material composed of copper, zinc, nickel and other alloys. Among them, the proportion of copper in its alloy is 60-98%, the proportion of zinc is 2-40%, and the proportion of nickel ranges from 0-5%. Copper alloy tape has good electrical conductivity and corrosion resistance, so it is widely used in electronics, manufacturing and other fields.

Characteristics of copper alloy coils

1. Good electrical conductivity: Copper alloy tape has good electrical conductivity, can effectively transmit current, and is suitable for high-frequency and high-speed circuits.

2. Good corrosion resistance: Copper alloy tape has excellent corrosion resistance and can be used for a long time in humid, acidic, high temperature and weathered environments without being easily damaged.

3. Good processing performance: Copper alloy coiled tape is easy to process and form, and can be made into coiled tapes with different precisions and sizes according to needs.

4. Low melting point: The melting point of copper alloy tape is lower than that of pure copper. It is easy to fuse and weld, and is convenient for making electronic components.

5. Good fatigue resistance: Copper alloy coil strip can withstand multiple bends without breaking easily. It has good fatigue resistance and is suitable for occasions that require frequent deformation.

Category:
The copper alloy plate and strip products include various grade of brass, red copper and tin/phosphor bronze series products, including H62, H65, H68, H70 and above brass products and QSn6.5-0.1 products. The company’s products cover common precision, precision and high precision copper plate and strip products.

Application of copper alloy coil

1. Electronic field: Copper alloy tape is widely used in the manufacturing of electronic components, such as inductors, capacitors, transformers, relays, etc.

2. Manufacturing field: Copper alloy tape can also be used to manufacture conductive connectors, springs, springs, contactors, force gauges, varistors, etc.

3. Construction field: Copper alloy coils and strips can be used as decorative materials in construction, such as elevator doors, doors and windows, etc.

[Conclusion] As a material with wide application value, copper alloy strip has good electrical conductivity and corrosion resistance. It has high application value in electronics, manufacturing, construction and other fields, and has broad market prospects.

1、Specifications

CategoryProductsGradesProduct StatusThicknessmmWidth

mm

Weight/unit

(kg)

Common StripCommon brass plate/stripH62 H65M、2M、3M、4M、TM、Y4、Y3、Y2、Y1、Y、2Y、TY、H and so on0.1~3.018~325≤600
H68 H700.1~3.018~305
Common phosphor copper stripQsn QF0.1~3.018~210≤250
High Precision StripHigh precision brass plate/stripH62 H65 H68
H70 H85 H90
0.08~2.610~420≤4000
High precision red copper plate/stripT20.1~2.610~420

2、Thickness Tolerance

Common StripBrass / phosphor copperSpecification (mm)Brass Tolerance(mm)Phosphor Copper Tolerance(mm)
≤0.2-0.01-0.02
0.21~0.39-0.015-0.025
0.40~0.8-0.02-0.04
0.81~1.5-0.04-0.05
1.51~2.0-0.05-0.06
2.01~2.5-0.06-0.06
High precision stripBrass/Red CopperSpecification(mm)Brass Tolerance(mm)Red Copper Tolerance(mm)
≤0.3±0.005±0.005
0.3~0.6±0.007±0.007
0.6~0.8±0.01±0.01
0.8~1.2±0.012±0.012
1.2~1.5±0.015±0.015
1.5~2.0±0.02±0.02
2.0~2.5±0.025±0.025

3、Mechanical Property

(1)Soft state mechanics standard

StateThickness/mmCommon Strip High Precision Strip
Cupping Test Value/mmCupping Test Value/mm
Soft Series0.10-0.16≥7.8≥7.8
0.17-0.19≥8.8≥8.8
0.2-0.24≥9.0≥9.0
0.30-0.35≥9.2≥9.4
0.36-0.41≥9.4≥9.6
0.42-0.45≥9.6≥9.8
0.51-0.54≥10.2≥10.2
0.55-0.59≥10.5≥10.5
0.60-0.90≥10.8≥10.7
≥1.0σb≥294N/mm2
δ≥48%
HV≤100
σb≥294
δ≥50%

(2)Hard State Mechanics Standard

ProductThickness/mmPropertyState
TY2YYY1Y2Y4
Common Strip0.10-0.19Cupping Test Valueσb≥560N/mm2
δ≥2.5%
——2.0-5.03.5-5.54.0-6.55.0-6.5
0.20-0.293.0-5.53.5-6.54.5-7.05.0-7.56.0-8.0
0.30-0.403.5-6.05.5-7.56.0-8.06.5-8.57.0-8.5
0.41-0.70σb/MPaσb≥430σb≥412372-471372-471σb≤430
δ/%δ:8-15%δ≥10%δ≥15%δ≥25%δ≥28%
≥0.71σb/MPaσb≥430σb≥412372-471372-471σb≤420
δ/%δ:8-15%δ≥10%δ≥15%δ≥25%δ≥30%
High Precision Strip0.10-0.19Cupping Test Valueσb≥588
MPa
δ≥2.5%
/2.0-5.03.5-5.54.0-6.55.0-6.5
0.20-0.293.0-5.53.5-6.54.0-6.55.0-7.56.0-7.5
0.30-0.403.5-6.05.5-7.56.0-8.06.5-8.57.0-8.5
≥0.2-0.4σb/MPa≥412≥400≥380360-400≤410
δ/%≥8≥1015-23≥23≥35
≥0.4-0.7σb/MPa≥430≥412≥412372-471≤420
δ/%8-15≥1015-23≥23≥35
≥0.7σb/MPa≥430≥412≥412372-471≤420
δ/%8-15≥1015-23≥30≥35

(3)Vickers Hardness

ProductMY4Y2Y1Y2YTY
Common Brass Strip80-10090-125110-135125-145140-160160-180180-200
High Precision Brass Strip75-90105-120115-130125-140145-160165-180185-200
High precision red copper alloy plate/strip50-6060-7090-105–100-115––