Incoloy® Alloy 020 Specifications
INCOLOY® alloy 020 is designated as UNS N08020.
Rod, Bar, Wire and Forging Stock: ASTM B 462, ASTM B 472, ASTM B 473, ASME SB 472, ASME SB 473, ISO 9723, ISO 9724, ISO 9725, DIN 17752-17754.
Plate, Sheet and Strip: ASTM A 240, ASTM A 480, ASTM B 463, ASTM B 906, ASME SA 240, ASME SA 480, ASME SB 463, ASME SB 906, ISO 6208, DIN 17750.
Pipe and Tube: ASTM B 729, ASTM B 829, ASTM B 468, ASTM B 751, ASTM B 464, ASTM B 775, ASTM B 474, ASME SB 729, ASME SB 829, ASME SB 468, ASME SB 751, ASME SB 464, ASME SB 775, ASME SB 474, ISO 6207, DIN 77751.
Other: – DIN 17744, ASTM B 366, ASTM B 462, ASTM B 471, ASTM B 475, ASME SB 366, ASME SB-462, ASME SB 471, ASME SB 475
Trademark Notice: Some names are trade names and/or trademarks of specific manufacturers. American Special Metals, Corp. is not affiliated with any manufacturer(s). Orders will be filled to meet specifications from any available source(s). Names are listed solely for reference to help identify products consistent with listed specifications.
Incoloy® Alloy 020 is a Registered Trademark of Special Metals Corporation and Its subsidiaries.
American Special Metals, Corp. makes all reasonable efforts to ensure the accuracy and correctness of the data in this document but makes no representations or warranties as to the data’s accuracy, correctness or reliability. All data are for general information only and not for providing design advice. It is the responsibility of the user to test specific alloys under actual service conditions to determine their suitability for a particular purpose.
Incoloy® Alloy 020 Introduction
Incoloy® Alloy 020 is an alloy composed of nickel-iron-chromium, with additions of molybdenum and copper. These alloys are categorized as super alloys and exhibit excellent corrosion resistance and high strength. Some of the INCOLOY alloys are specifically made to resist selected reagents. These alloys are capable of functioning even at high temperatures.
INCOLOY alloy 020 exhibits excellent corrosion resistance in chemical environments that contain sulphuric acid, chlorides, phosphoric acid and nitric acid. It is easy to fabricate this alloy to form mixing tanks, heat exchangers, pickling equipment etc. The standard forms in which this alloy is available are round, flats, pipe, tube, strip and wire.
This datasheet will look into the chemical composition, properties and applications of INCOLOY 020.
Incoloy® Alloy 020 Chemical Composition
The chemical composition of INCOLOY alloy 020 is given in the following table.
| Element | Content (%) |
|---|---|
| Nickel, Ni | 32-38 |
| Iron, Fe | 35 |
| Chromium, Cr | 19-21 |
| Copper, Cu | 3-4 |
| Molybdenum, Mo | 2-3 |
| Manganese, Mn | ≤2 |
| Niobium, Nb | ≤1 |
| Silicon, Si | ≤1 |
| Others | Remainder |
Incoloy® Alloy 020 Physical Properties
The following table discusses the physical properties of INCOLOY alloy 020.
| Properties | Metric | Imperial |
|---|---|---|
| Density | 8.05 gm/cm3 | 0.291 lb/in3 |
Incoloy® Alloy 020 Mechanical Properties
The mechanical properties of INCOLOY alloy 020 are tabulated below.
| Properties | Metric | Imperial |
|---|---|---|
| Tensile strength(annealed) | 620 MPa | 89.9 ksi |
| Yield strength(annealed) | 300 MPa | 43.5 ksi |
| Elongation at Break | 41% | 41% |
Some of the designations used to denote INCOLOY alloy 020 are listed below:
- UNS N08020
- ASME SB-462 – SB 464
- ASME SB 468
- ASTM B 462
- ASTM B 464
- ASTM B 472
- ASTM B 474
- ASTM B 751.
Incoloy® Alloy 020 Fabrication
Welding
Incoloy® Alloy 020 can be welded by shielded metal arc welding, gas tungsten arc welding and gas metal arc welding. The filler metal is usually an INCONEL alloy.
Hot Working
Incoloy® Alloy 020 can be hot worked at temperature ranges of 760-1175°C (1400-2150°F).
Annealing
Incoloy® Alloy 020 should be annealed at 982-1010°C (1800-1850°F) for time commensurate with section size /AC.
Applications
The Incoloy® Alloy 020 is used in the following applications:
- Produce mixing tanks, heat exchangers, valves, fittings and fasteners
- Production of gasoline, solvents, explosives and organic chemicals
- Pharmaceuticals and food industry.