Alloy 254 SMO® / 1.4547 / UNS S31254

Alloy 254 SMO® is an austenitic stainless steel alloy with 6% molybdenum and nitrogen. It has a very high resistance to crevice and surface corrosion. Alloy 254 SMO® was specially developed for the pulp and paper industry and for offshore use on oil and gas platforms.

Alloy 254 SMO® / 1.4547 / UNS S31254 metal powder for 3d metal printing

We are pleased to offer you powder for 3D printing made of Alloy 254 SMO® / 1.4547 / UNS S31254. Send us your inquiry.

Category:

General characteristics

Ultra 254 SMO® is a 6% molybdenum and nitrogen-alloyed austenitic stainless steel with extremely high resistance to both uniform and localized corrosion. This product was developed especially for oil and gas offshore platforms and the pulp and paper industry.

Typical applications

  • Applications requiring resistance to chlorinated seawater
  • Flue gas cleaning
  • Maritime exhaust gas cleaning (EGC)
  • Bleaching equipment in the pulp and paper industry
  • Flanges and valves

254 SMO® Chemical composition

The typical chemical composition for this grade is given in the table below, together with composition limits given for the product according to different standards. The required standard will be fully met as specified on the order.

The chemical composition is given as % by mass.

StandardGradeCMnCrNiMoNOther
Typical254 SMO®0.0120.018.06.10.20Cu:0.7
ASME II A SA-240UNS S31254≤0.020≤1.0019.50-20.5017.50-18.506.00-6.500.18-0.25Cu:0.50-1.00
ASTM A240UNS S31254≤0.020≤1.0019.5-20.517.5-18.56.0-6.50.18-0.25Cu:0.50-1.00
EN 10028-71.4547≤0.020≤1.0019.5-20.517.5-18.56.0-7.00.18-0.25Cu:0.50-1.00
EN 10088-21.4547≤0.020≤1.019.5-20.517.5-18.56.0-7.00.18-0.25Cu:0.5-1.0
EN 10088-31.4547≤0.020≤1.0019.5-20.517.5-18.56.0-7.00.18-0.25Cu:0.50-1.00
EN 10088-41.4547≤0.020≤1.019.5-20.517.5-18.56.0-7.00.18-0.25Cu:0.5-1.0
IS 6911ISS 312≤0.020≤1.0019.5-20.517.5-18.56.0-6.50.18-0.25Cu:0.50-1.00
StandardGradeCMnCrNiMoNOther

254 SMO® Mechanical properties

The addition of nitrogen to Ultra 254 SMO® gives higher proof strength and tensile strength. Despite the greater strength, the possibilities for cold as well as hot forming are very good.

Mechanical properties at room temperature are shown in the table below.

StandardGradeRp0.2Rp1.0RmElongationImpact strengthRockwellHBHV
MPaMPaMPa%J
Product type: Cold rolled coil and sheet
Typical (thickness 1 mm)37541573560
ASME II A SA-240UNS S31254≥ 310≥ 655≤ 223
ASTM A240UNS S31254≥ 310≥ 655≤ 96HRB≤ 223
EN 10028-71.4547≥ 320≥ 350650-850≥ 35
EN 10088-21.4547≥ 320≥ 350650-850≥ 35
EN 10088-41.4547≥ 320≥ 350650-850≥ 35
IS 6911ISS 312≥ 310≥ 690≤ 96HRB≤ 223
Product type: Hot rolled coil and sheet
Typical (thickness 4 mm)
ASME II A SA-240UNS S31254≥ 310≥ 655≤ 223
ASTM A240UNS S31254≥ 310≥ 655≤ 223
EN 10028-71.4547≥ 320≥ 350650-850≥ 35
EN 10088-21.4547≥ 320≥ 350650-850≥ 35
EN 10088-41.4547≥ 320≥ 350650-850≥ 35
IS 6911ISS 312≥ 310≥ 690≤ 96HRB≤ 223
Product type: Hot rolled quarto plate
Typical (thickness 15 mm)32035068050160
ASME II A SA-240UNS S31254≥ 310≥ 655≤ 96HRB≤ 223
ASTM A240UNS S31254≥ 310≥ 655≤ 96HRB≤ 223
EN 10028-71.4547≥ 300≥ 340650-850≥ 40
EN 10088-21.4547≥ 300≥ 340650-850≥ 40
EN 10088-41.4547≥ 300≥ 340650-850≥ 40
IS 6911ISS 312≥ 310≥ 655≤ 96HRB≤ 223
Product type: Wire rod
Typical34038068050
StandardGradeRp0.2Rp1.0RmElongationImpact strengthRockwellHBHV
MPaMPaMPa%J

1)Elongation according to EN standard: A80 for thickness below 3 mm. A for thickness = 3 mm. Elongation according to ASTM standard A2” or A50.

Corrosion resistance

Uniform corrosion

The high content of alloying elements gives Ultra 254 SMO® exceptionally good resistance to uniform corrosion. It can withstand a wide range of acids due to the high alloying content of chromium and molybdenum. For guidance on material selection in a large number of environments, consult the tables and isocorrosion diagrams in the Outokumpu Corrosion Handbook.

Pitting and crevice corrosion

Resistance to pitting and crevice corrosion is determined mainly by the chromium, molybdenum, and nitrogen content. Ultra 254 SMO® has high amounts of these elements and is suitable for demanding environments like chlorinated sea water.

Stress corrosion cracking

Resistance to stress corrosion cracking increases with increased content of nickel and molybdenum in particular. This means that Ultra 254 SMO® has very good resistance to stress corrosion cracking.

Pitting corrosion resistanceCrevice corrosion resistance
PRECPTCCT
4387±335
Pitting corrosion resistanceCrevice corrosion resistance
PRECPTCCT

PRE Pitting Resistant Equivalent calculated using the formula: PRE = %Cr + 3.3 x %Mo + 16 x %NCPT Corrosion Pitting Temperature as measured in the Avesta Cell (ASTM G 150), in a 1M NaCl solution (35,000 ppm or mg/l chloride ions).CCT Critical Crevice Corrosion Temperature is the critical crevice corrosion temperature which is obtained by laboratory tests according to ASTM G 48 Method F

Physical properties

The typical values of some physical properties are given in the table below.

DensityModulus of elasticityThermal exp. at 100 °CThermal conductivityThermal capacityElectrical resistanceMagnetizable
kg/dm3GPa10-6/°CW/m°CJ/kg°CµΩm
8.019516,5145000.85No*
DensityModulus of elasticityThermal exp. at 100 °CThermal conductivityThermal capacityElectrical resistanceMagnetizable
kg/dm3GPa10-6/°CW/m°CJ/kg°CµΩm

*) Austenitic stainless steel grades may be magnetizable to a certain degree after cold deformation, e.g. in temper rolled condition.

Fabrication

Ultra 254 SMO® cold hardens considerably faster than conventional austenitic grades. This, together with the initial high strength, makes it necessary to apply high forming forces. The springback for Ultra 254 SMO® is also greater than for conventional austenitic steels. In complicated cold forming operations, intermediate annealing of the material may sometimes be necessary, especially if the workpiece is welded.

Machining

The work hardening behavior together with the toughness means that highly alloyed grades are often perceived as problematic from a machining perspective, e.g. operations such as turning, milling, and drilling. This applies to an even greater extent to most highly alloyed steels, especially those that have a high nitrogen content. However, with the right choice of tools, tool settings, and cutting speeds, these materials can be sucessfully machined. Machining guidelines for Ultra 254 SMO® can be found here :Machining guidelines Ultra 254 SMO®

Welding

Ultra 254 SMO® is well suited for welding, and the methods used for welding conventional austenitic steels can be used. However, due to its stable austenitic structure, it is somewhat more sensitive to hot cracking in connection with welding, and generally welding should be performed using a low heat input. On delivery, sheet, plate, and other processed products have a homogeneous austenitic structure with an even distribution of alloying elements in the material. Solidification after partial remelting, e.g. by welding, causes redistribution of elements such as molybdenum, chromium, and nickel. These variations, segregation, remain in the cast structure of the weld and can impair the material’s corrosion resistance in certain environments.

More detailed information concerning welding procedures can be obtained from the Outokumpu Welding Handbook, available from our sales offices.

More detailed information concerning welding procedures can be obtained from the Outokumpu Welding Handbook, available from our sales offices.

254 SMO® Standards & approvals

The most commonly used international product standards are given in the table below.

StandardDesignation
ASME SA-240M Code Sect. II. Part AUNS S31254 / 254
ASTM A240/A240MUNS S31254 / 254
EN 10028-7 (PED 2014/68/EU)1.4547
EN 10088-21.4547
EN 10088-31.4547
EN 10088-41.4547
IS 6911, AMENDMENT NO. 3ISS 312
StandardDesignation