Characteristic Aluminum Bronze Tin Bronze Composition Main Alloying Element Aluminum (5-12%) Tin (5-25%) Other Common Elements Iron, Nickel, Manganese, Silicon Phosphorus, Lead, Zinc Typical Grades C95200 (Cu-9Al-2Fe)C95400 (Cu-11Al-4Fe)C95500 (Cu-11Al-4Ni-4Fe) C90700 (Cu-10Sn)C93200 (Cu-7Sn-7Pb-2Zn)C52100 (Cu-8Sn-0.3P) Physical Properties Color Golden to reddish-gold Reddish to pale yellow Density 7.7-8.1 g/cm³ 8.7-8.9 g/cm³ Melting Point 1030-1080°C (1886-1976°F) 830-1000°C (1526-1832°F) Thermal...
Tin bronze and aluminum bronze are both types of copper alloys, but they differ in their composition and properties: Composition: Properties: Applications: In summary, the main differences lie in their alloying elements and resulting mechanical and corrosion-resistant properties, which dictate their respective applications.