Inconel C263 and Hastelloy C276 are both high-performance nickel-based superalloys, each with unique properties that make them valuable in different industrial applications. This comparison highlights the key differences between these two alloys, including their chemical composition, mechanical properties, temperature performance, and typical uses. Understanding these distinctions is crucial for engineers and designers when selecting materials for specific projects, particularly those involving high temperatures or corrosive environments. Let’s examine these alloys in detail:

Chemical Composition (nominal, weight %)

ElementInconel C263Hastelloy C276
NickelBalanceBalance
Chromium19-2114.5-16.5
Molybdenum5.6-6.115-17
Cobalt19-212.5 max
Tungsten–3-4.5
Iron0.7 max4-7
Titanium1.9-2.4–
Aluminum0.3-0.6–

Mechanical Properties (typical)

PropertyInconel C263Hastelloy C276
Tensile Strength (MPa)850-1050690-930
Yield Strength (MPa)550-680280-360
Elongation (%)25-4050-60
Hardness (Brinell)220-270190-230

Temperature Performance

AspectInconel C263Hastelloy C276
Max Service Temp (°C)8501100
Oxidation ResistanceExcellentVery Good

Corrosion Resistance

EnvironmentInconel C263Hastelloy C276
OxidizingExcellentExcellent
ReducingGoodExcellent
Pitting/CreviceVery GoodExcellent

Key Features

Inconel C263:

  • High strength at elevated temperatures
  • Good oxidation resistance
  • Excellent creep resistance
  • Used in gas turbine components, exhaust systems

Hastelloy C276:

  • Exceptional corrosion resistance in a wide range of environments
  • Excellent resistance to pitting and stress corrosion cracking
  • Good fabricability and weldability
  • Used in chemical processing, pollution control, pulp and paper production

Typical Applications

Inconel C263:

  • Gas turbine components (combustion cans, transition ducts)
  • High-temperature fasteners
  • Heat shields
  • Exhaust systems

Hastelloy C276:

  • Chemical processing equipment
  • Flue gas desulfurization systems
  • Offshore oil and gas components
  • Nuclear waste treatment facilities

Weldability

AspectInconel C263Hastelloy C276
WeldabilityGoodExcellent
Post-weld Heat TreatmentRequiredNot typically required