Wear Resistant Steel Plate is a special plate product specially designed for use under large area wear conditions. The commonly used wear-resisting steel plate is made of the alloy wear-resisting layer with high hardness and good wear resistance compounded by surfacing method on the surface of ordinary low carbon steel or low-alloy steel with good toughness and plasticity. In addition, there are cast wear-resistant steel plates and alloy hardened wear-resistant steel plates.

Aplikasi

Wear-resistant steel plate has high wear-resistant performance and good impact performance, can be cut, bend, welding, welding, bolt connection and other ways to connect with other structures, in the maintenance site process has the characteristics of saving time, convenient, widely used in metallurgy, coal, cement, electric power, glass, mining, building materials, brick and other industries, compared with other materials, With high cost performance, it has been favored by more and more industries and manufacturers.

Kategori:
Resistant Steel Plate Standards:

  • NM360, WUSTEEL, NM450, NM500
  • NR360, NR400
  • B-HARD360, B-HARD400, B-HARD450
  • KN-55, KN-60, KN-63
  • AR400, AR450, AR500, AR600

Plat NM400

Wear/Abrasion Resistant Steel Equivalent Standards

adalah Baja Struktural Kekuatan Tinggi Paduan Rendah Standar GB CinaPerbandingan pelat baja tahan aus WNM400 dan baja imporJFEDILLIDURThyssenkKruppRuukki
NM360-EH360---
WUSTEELPerbandingan pelat baja tahan aus WNM400 dan baja imporEH400400VXAR400Raex400
NM450HARDOX450-450VXAR450Raex450
NM500HARDOX500EH500500VXAR500Raex500

Wear/Abrasion Resistant Steel — Chinese Standard

NM360 WUSTEEL NM450 NM500 NR360 NR400 B-HARD360 B-HARD400 B-HARD450 KN-55 KN-60 KN-63

Chemical Composition (%) of NM Wear Resistant Steel
adalah Baja Struktural Kekuatan Tinggi Paduan Rendah Standar GB CinaCDanM NPSCrMoBadalah Baja Struktural Kekuatan Tinggi Paduan Rendah Standar GB CinaHCeq
NM360/NM4000.200,401,50≤0.0120,005≤0.350.300,0020,005≤0.00025≤0.53
NM450≤0.220,601,50≤0.0120,0050,800.300,0020,005≤0.00025≤0.62
NM5000.300,60Huruf pertama dari pinyin Cina dari karakter≤0.0120,002Huruf pertama dari pinyin Cina dari karakter0.300,0020,005≤0.0002≤0.65
NM550≤0.350,40≤1.200.0100,002Huruf pertama dari pinyin Cina dari karakter0.300,002≤0.0045≤0.0002≤0.72
Mechanical Properties of NM Wear Resistant Steel
adalah Baja Struktural Kekuatan Tinggi Paduan Rendah Standar GB CinaYield Strength /MPaTensile Strength /MPaPemanjangan A50 /%Hardess (Brinell) HBW10/3000Impact/J (-20℃)
NM360≥900≥105012320-390= Tebal atau diameter kawat dalam mm
WUSTEEL≥950≥120012380-430= Tebal atau diameter kawat dalam mm
NM450≥1050≥1250≥7420-480= Tebal atau diameter kawat dalam mm
NM500≥1100≥1350≥6≥470= Tebal atau diameter kawat dalam mm
NM550---≥530-

Wear/Abrasion Resistant Steel — USA Standard

AR400 AR450 AR500 AR600
Abrasion Resistant Steel Plate Availabillity
NilaiKetebalanLebarPanjang
AR200 / AR 2353/16″ – 3/4″48″ – 120″96″ – 480″
AR400F3/16″ – 4″48″ – 120″96″ – 480″
AR450F3/16″ – 2 “48″ – 96 “96″ – 480″
AR5003/16″ – 2 “48″ – 96 “96″ – 480″
AR6003/16″ – 3/4″48″ – 96 “96″ – 480″
Chemical Composition of Abrasion Resistant Steel Plate
NilaiCDanM NPSCrNiMoB
AR5000.300.71.700.0250.0151.000.700.500.005
AR4500.260.71.700.0250.0151.000.700.500.005
AR4000.250.71.700.0250.0151.500.700.500.005
AR3000.180.71.700.0250.0151.500.400.500.005
Mechanical Properties of Abrasion Resistant Steel Plate
NilaiYield Strength MPaTensile Strength MPaPerpanjangan AImpact Strength Charpy V 20JHardness Range
AR500125014508-30C450-540
AR450120014508-40C420-500
AR4001000125010-40C360-480
AR300900100011-40C-

Abrasion Resistant Steel Plate Applications:

  • The AR235 plates are intended for moderate wear applications where it offers improved wear resistance relative to structural carbon steel.
  • The AR400 are premium abrasion resistant steel plates that are heat-treated and exhibit through-hardening. Improved forming and weding capabilities.
  • AR450 is an abrasion resistant plate used in a variety of applications where slightly greater strength is desired beyond AR400.
  • AR500 plates are suitable for mining, forestry and construction applications.
  • AR600 is utilized in high-wear areas such as aggregate removal, mining, and the manufacture of buckets and wear bodies.

Abrasion Resistant (AR) steel plate is typically made in the as-rolled condition. These types/grades of steel plate products have been developed specifically for long service life in harsh conditions. AR products are suitable for a variety of applications in areas such as mining/quarrying, conveyors, material handling and construction, and earthmoving. Designers and plant operators choose AR plate steel when striving to extend service life of critical components, and reduce the weight of each unit put into service. The benefits of employing wear-resistant plate steel in applications involving impact and/or sliding contact with abrasive material are immense.

Abrasive resistant alloy steel plates generally offer good resistance to sliding and impact abrasion. The high carbon content in the alloy increases the hardness and toughness of the steel, making it an ideal material for applications that require high impact or high abrasion resistance. It is possible to get high hardness with a high carbon steel, and the steel will have good resistance to penetration. However, the wear rate will be rapid compared to heat treated alloy plate because high carbon steel is brittle, so particles can be more easily torn from the surface. As a result, high carbon steels are not used for high wear applications.