Deskripsi Baja Alat P20

P20 die steel is a kind of mold welding material model, the earliest is P20, followed by P20H, P20Ni have come out. P20 steel is suitable for making plastic molds and die casting of low melting point metals. This steel has good machinability and mirror abrasive properties.

Prehardened plastic die steel. Widely used in China, factory hardness HRC30~42, suitable for large and medium-sized precision molds, suitable for long-term production of high quality plastic molds, used for large mold frame. This steel has good machinability and general polishing ability.

Spesifikasi Baja Alat P20 yang Relevan dan Kelas Baja Setara

NegaraAmerika SerikatJermanGB/T
StandarASTM A681DIN EN ISO 4957GB/T 1299
NilaiP201.23113Cr2Mo

Baja Perkakas P20 (baja cetakan plastik) Bahan kimia Komponen

C
Dan
M N
P
S
Cr
Mo
Ni
0.28-0.4
0.2-0.8
0.6-1
0.03
0.03
1.4-2
0.3-0.55
0.05-0.10

Kategori: Tag:

Baja Perkakas P20 (baja cetakan plastik)


LION METAL is ASTM P20 Tool Steel stockholders and suppliers from china(Shanghai). we have more our 26 years experience in special steel supply.

ASTM P20 Steel is a good quality plastic tool steel, P20 steel belong to the high quality medium carbon,Pre-hardness(28~34HRc) plastic mould steel. It no need further heat treatment. so you don’t have any worry about distortion or cracking.

Spesifikasi Baja Alat P20 yang Relevan dan Kelas Baja Setara

NegaraAmerika SerikatJermanGB/T
StandarASTM A681DIN EN ISO 4957GB/T 1299
NilaiP201.23113Cr2Mo

P20 Steel Properties Related Specifications ASTM A681-1999 | JIS G4404(2000) | GB 1299


Bahan Plat Baja AISI P20

ASTM A681CM NPSDanCrMo
P200.280.40.610.030.030.20.81.420.30.55
DIN ISO 4957CM NPSDanCrMo
1.23110.350.451.31.60.030.030.20.41.82.10.150.25
GB/TCM NPSDanCrMo
GBT 12990.280.40.610.030.030.20.81.420.30.55

Bentuk Pasokan

ASTM P20 tool steel, we can supply the p20 steel round bar, steel flat bar, steel plate, hexagonal steel bar and steel square block. P20 steel Round bar can be sawn to your required lengths as one offs or multiple cut pieces. Rectangular pieces can be sawn from flat bar or plate to your specific sizes. Ground tool steel bar can be supplied, providing a quality precision finished bar to tight tolerances.

Aplikasi

ASTM P20 Tool steel is a American plastic Die steel material, the steel by “super clean” production process, pre hardened, showing the height of micro pure and excellent homogeneous structure, excellent polishing and light etching engraving.

After heat treatment, processing and polishing performance is good, can be carried out, and can be processed, suitable for the surface treatment of chrome, material hardness, good toughness, good mechanical processing performance.

Gold microstructure is martensite and bainite structure.

Main be applied to in plastic steel mold. like car injection moulding, PVC plastic injection molding.


Ukuran reguler dan Toleransi

Batang bundar: Diameter Ø 5mm – 3000mm

Pelat: Tebal 5mm – 3000mm x Lebar 100mm – 3500mm

Flat bar: 5mm – 105mm

1. Hot Rolled round bar

Diameter
(mm)
Toleransi Diameter
(mm)
Diameter
(mm)
Toleransi Diameter
(mm)
12.70-0.13~0.30>50.80~63.5-0.25~0.76
12.7~25.40-0.13~0.41>63.50~76.20-0.25~1.02
>25.4~38.10-0.15~0.51>76.20~101.60-0.30~+1.27
>38.1~50.80-0.20~0.64>101.60~203.20-0.38~3.81

2. Hot Rolled steel plate

Ketebalan
(mm)
Toleransi Ketebalan
(mm)
Ketebalan
(mm)
Toleransi Ketebalan
(mm)
25.4-0,41~0,79>127~152-1,60~2,39
>25,4~76-0,79~1,19>178~254-1,98~3,18
>76~127-1.19~1.60>254~305-2.39~3.96

Yang lain belum menentukan ukuran, harap hubungi tim penjualan kami yang berpengalaman.


Properti

  1. The vacuum degassing refining treatment of pure steel, suitable for polishing or etching processing plastic mold.
  2. Pre-hard state supply, no need in the heat treatment can be directly used for mold processing, shorten the construction period.
  3. After forging and rolling processing, the structure is compact, 100% ultrasonic inspection, no pores, needle hole defects.

USES:

  1. Thermoplastic injection mold, extrusion mold.
  2. Thermoplastic plastic blow mold.
  3. Heavy duty mold main parts.
  4. Cold structure parts.
  5. Commonly used in the manufacture of TV case, washing machine, refrigerator shell, bucket, etc.

Pengolahan

(1) Round bar and flat sections can be cut to your required sizes.

(2) Round bar can also be supplied, providing a high quality tool steel precision ground tool steel bar to your required tolerances.

(3) Is also available as Ground Flat Stock / Gauge Plate, in standard and nonstandard sizes.

Penempaan baja cetakan plastik bahan baja AISI P20

Slowly Heat to 930-1050 °C, keep the temperature to heat thoroughly. Start forging. Finished cool slowly.


Annealing dari bahan baja alat cetakan plastik Din P20

Heat to 775 to 790 °C, soak enough time, ensure heat thoroughly. then cool in the heat treatment furnace.

Pendinginan bahan p20

820-840°C, quench in oil. get p20 steel material hardness 28~34HRc


Tempering bahan kelas baja cetakan plastik P20

Heat uniformly at the tempering temperature for P20 tool steel material. keep enough time, then cool in air.

Advice temperature 100 to 600°C. more P20 mold tool steel heat treatment data, pls contact your heat treatment supplier,.


Hubungi tim penjualan kami yang berpengalaman untuk membantu Anda dengan pertanyaan baja Alat P20 Anda

by Email or Telphone. The P20 Steel questions will be reply in 24 hours.