Profil baja JFE Jepang

JFE Steel memiliki sejarah 90 tahun dan merupakan salah satu dari 10 perusahaan baja terbaik di dunia.

Berdasarkan pengalaman, penelitian dan pengembangannya, baja JFE telah melakukan upaya tak henti-hentinya untuk meningkatkan peralatan, meningkatkan variasi, dan memperkaya manajemen kualitas setiap tahun untuk memenuhi kebutuhan pelanggan kami.

Di Jepang, baja JFE dengan tiga pabrik pelat medium tercanggih di dunia, dapat memproduksi produk pelat medium dengan lebar 5350 mm dan tebal 360 mm, seperti baja berkekuatan tinggi, baja tahan aus, pelat baja suhu rendah, ketel, pelat baja bejana tekan, pelat baja tahan korosi atmosfer kelas atas nikel, pelat baja tahan karat, semua jenis pelat baja komposit, dll., produksi lebih dari jutaan ton.

Seri pelat baja tahan aus JFE

  • EH-C340, C400, C450, C500, C550
  • EH-C400LE, C450LE, C500LE

Seri pelat baja kekuatan tinggi JFE

  • HITEN780S, 780LE
  • HITEN980S
  • HYD960LE

Kategori: Menandai:

Lion metal is a leading wholesaler vendor, merchant, and exporter of JFE EH C400 Plates.

We also manufacture all the household stainless steel, high nickel alloys, and carbon steel C400 Plates are designed with a chemical composition like carbon, chromium, boron, molybdenum, manganese, phosphorous, silicon, nickel, and sulfur.

Also, these plates are made with mechanical properties such as yield strength, tensile strength, elongation, and longitudinal degrees.

JFE EH C400 plates include some of the specifications such as heat treatment, material types, Brinell hardness, and various grades.

C400 plates are applicable in many industries like machine building, lifting & mobile equipment, stone & iron chutes, framework structures, pylons & wearing plates, containers, truck frames, rail cars, crane booms, anti-drill plates like tumbling machine, shot blasting equipment, security doors, and stone crusher.

Pelat Baja JFE EH C400 are also helpful in some purposes like dump truck bodies, loading buckets, bulldozers, and conveyors. This plate has found various applications like material and important parts of building & bridge construction, transport, and mining types of machinery.

EH C400 plates are precisely suitable for extreme atmosphere with high toughness, low temperatures, and resistant from high impact conditions of the plate. These plates are helpful in abrasion resistance, workability, and weldability.

These plates are also resistant to the safety of welded joints, and weld cracking. C400 is developed with the highly resistant from abrasion as compared to C500 plates.

Pelat JFE EVERHARD C400 are mainly considered for the low-temperature toughness. These products are long-lasting as well as increase the formability and higher abrasion resistant plates.

Brinell hardness at the plate makes the plate low-temperature toughness. EH C400 plates are extremely more abrasion resistant than the regular steels. They are lighter in weight and contribute to the atmosphere.

These plates are useful in extreme cold conditions. These plates even enable low welding temperature craking.

JFE EH C400 Plates undergo many tests after production such as hydrostatic test:

Intragranular test, mechanical tests, Charpy test, hardness test, chemical test, tensile test, destructive test, flaring test, flattening test, Spectro test, blaze test, corrosion test, ultrasonic test, radiography test, pitting resistance test and many more.

JFE EH C400 Plate Specification :

  • Barang: Pelat Tahan Abrasi
  • Ketebalan: 5 – 50,8, 50,9 – 101,6
  • Panjang : 1.0000 mm hingga 12.000 mm
  • Lebar : 500mm hingga 3000mm
  • Permukaan : Tempering, Quenched, Normalisasi.
  • Sertifikat: ISO9001:2000
  • Produksi : Canai Panas (HR) / Canai Dingin (CR)
  • Aplikasi : industri beton, metalurgi, industri kipas angin, industri batubara, mesin pertambangan, mesin konstruksi, dll.
  • Perlakuan panas: Perlakuan panas terkontrol

JFE EH C400 PLATES KIMIA KOMPOSISI

NilaiCDanM NPSCrMoVAndaBCeq**
JFE EH C40000,20 maks----0.40 – 1.2000,50 maks-00,020 maks.00,004 maks.-

SIFAT MEKANIK PIRING JFE EH C400

Nama merkKetebalan (mm)Kekerasan Brinell [dijamin] (29,42 kN) Rata-rata 5 poinSifat dampak Charpy (2mmV)Ceq (%)**
[terjamin]
Suhu pengujian [dijamin] (C°)Charpy menyerap energi (J) [dijamin]*
EVERHARD-C4505 – 101.6450±25---