This article compares the characteristics of UNS C63200 and UNS C95800 copper alloys, detailing their chemical compositions, mechanical properties, performance at different temperatures, industry applications, shape, size, production standards, and additional relevant factors.
Chemical Composition
Element
C63200 (%)
C95800 (%)
Aluminum (Al)
8.7 – 9.5
8.5 – 9.5
Nickel (Ni)
4.0 – 4.8
4.0 – 5.0
Iron (Fe)
3.5 – 4.3
3.5 – 4.5
Manganese (Mn)
1.2 – 2.0
0.8 – 1.5
Silicon (Si)
0.1
0.1
Lead (Pb)
0.02
0.03
Copper (Cu)
Balance
79
Mechanical Properties
Property
C63200
C95800
Hardness (Rockwell B)
85-95
85-90
Tensile Strength
550 MPa
620 MPa
Yield Strength
300 MPa
380 MPa
Elongation at Break
10%
8%
Elastic Modulus
117 GPa
117 GPa
Charpy Impact
25.0 J
15.0 J
Machinability
70
40
Performance at Different Temperatures
Property
C63200
C95800
Melting Point
1033°C (1911°F)
1060°C (1940°F)
Thermal Conductivity
50.0 W/mK (346 BTU in/hr.ft²°F)
40.0 W/mK (276 BTU in/hr.ft²°F)
Thermal Expansion Coefficient
16.3 µm/m°C
16.5 µm/m°C
Industry Applications
Application
C63200
C95800
Marine Components
Yes
Yes
Pump and Valve Components
Yes
Yes
Electrical Connectors
Limited
Limited
Heavy Machinery Parts
Limited
Yes
Shape and Size
Attribute
C63200
C95800
Available Shapes
Rods, Bars
Rods, Bars
Standard Sizes
Various
Various
Common Forms
Sheet, Plate
Sheet, Plate
Production Standards
Standard
C63200
C95800
ASTM
B505, B150
B505, B150
ASME
SFA 5.7
SFA 5.7
SAE
J461, J463
J461, J463
Welding and Processing
Processing Method
C63200
C95800
Welding Compatibility
Good (with precautions)
Limited
Preferred Welding Method
Gas shielded, resistance
Somewhat difficult
Polishing
Good polishing capability
Moderate polishing capability
Heat Treatment
Yes
Yes
Cold Processing
Moderate capacity
Limited
Advantages and Disadvantages
Attribute
C63200
C95800
Advantages
Good strength, corrosion resistant
Excellent wear resistance, high strength
Disadvantages
Lower wear resistance compared to C95800
Higher cost, lower machinability
Similar Products
Similar Products
Properties
Copper Nickel Alloys
Good corrosion resistance, suitable for marine applications.
Aluminium Bronze Alloys
High strength and corrosion resistance, often used in similar applications.
Comparison of Similar Products
Product
Corrosion Resistance
Strength
Applications
UNS C63200
High
Moderate
Marine, Pumps, Valves
UNS C95800
Higher
High
Pumps, Heavy Machinery
Copper Nickel Alloys
Very High
Moderate
Marine, Plumbing
Conclusion
In conclusion, both UNS C63200 and UNS C95800 copper alloys exhibit unique properties that make them suitable for different applications. C63200 is characterized by its good strength and corrosion resistance, making it a reliable option for marine components. In contrast, C95800 provides superior wear resistance and is better suited for high-stress applications, particularly in heavy machinery. Understanding these distinctions will facilitate informed choices in material selection for various engineering requirements. If you have any further questions or need additional information, feel free to ask!
International Standard Mapping Comprehensive Equivalency Comparison Country Standard Code Alloy Designation Composition Similarity Performance Match...
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional
Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes.The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.