Dillidur 500 Description

Dillidur 500 is a wear-resistant steel plate with a nominal hardness of 500 HBW in the delivery state.

Dillidur 500 is recommended for applications in extremely high-wear environments where materials are required to have excellent machinability, especially excellent welding performance.

Contoh aplikasi: jentera pengangkut tanah, jentera pemuatan, kapal korek, trak pembuangan, peralatan pengangkutan, trak pembuangan, bilah, penghancur potong, peralatan rawatan sisa dan kitar semula, dsb.

Dillidur 500 Wear-Resistant Steel Plate

DILLIDUR 500 is a wear-resistant steel plate with a nominal hardness of 500 HBW in the delivery state.

DILLIDUR 500 is recommended for applications in extremely high-wear environments where materials are required to have excellent machinability, especially excellent welding performance.

Contoh aplikasi: jentera pengangkut tanah, jentera pemuatan, kapal korek, trak pembuangan, peralatan pengangkutan, trak pembuangan, bilah, penghancur potong, peralatan rawatan sisa dan kitar semula, dsb.

DILLIDUR 500 Product Description

Supply size range

According to the supply outline, DILLIDUR 500 is available in thicknesses from 8mm (1/3 inch) 2 hingga 100mm (4 inci) 2 . Other size requirements can be discussed separately.

DILLIDUR 500 Chemical Composition:

Berdasarkan analisis peleburan, nilai had (%) berikut boleh digunakan untuk setiap komponen

CDanMnPS
≤ 0.30≤ 0.70≤ 1.60≤ 0.025≤ 0.010

Bergantung pada ketebalan, satu atau lebih unsur pengaloian berikut akan ditambah:

MoDalamCuCrVNbB
≤ 0.50≤ 1.0≤ 0.30≤ 1.50≤ 0.08≤ 0.05≤ 0.005

Keluli lebur ditenangkan sepenuhnya dan diproses untuk butiran halus.

Nilai rujukan setara karbon:

Steel plate thickness [mm]104080CEV a0.530.570.67CET b0.390.410.44

a CEV =C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15

b CET =C+(Mn+Mo)/10+(Cr+Cu)/20+Ni/40

1 The content of this information is a product description, and may be updated from time to time.

2 The approximate conversion value in parentheses is an offensive reference.

Status penghantaran:

Pelindapkejutan air terkawal suhu

Sifat mekanikal dalam keadaan penghantaran

Kekerasan

Brinell hardness of surface at room temperature:

Board thickness ≤ 30mm (1.2 inches) 3 , 470-530 HBW

Board thickness> 30mm (1.2 inches) 3 , 450-530 HBW

Ujian tegangan spesimen melintang pada suhu bilik (nilai rujukan untuk plat keluli tebal 20mm)

Tensile strength: 1600 MPa (232 ksi) 3

Yield point: 1100 MPa (160 ksi) 3

Elongation: 9% (L o = 5.65 √S o )

Although DILLIDUR has high tensile properties, it is not suitable for applications that emphasize safety. In this case, please use high-strength steel DILLIMAX.

Spesimen longitudinal V-notch Ujian hentaman Charpy (nilai rujukan untuk plat keluli tebal 20mm)
Charpy impact energy: 25 J at -20°C (-4°F) 3

The Brinell hardness of the test surface is tested every furnace and every 40 tons.

Tanda plat keluli
Jika tiada perjanjian lain, tanda plat keluli hendaklah mengandungi sekurang-kurangnya kandungan berikut:

  • Grade (DILLIDUR 500)
  • Nombor relau
  • Nombor papan induk dan nombor plat keluli
  • Tanda kilang keluli
  • Tandatangan Inspektor

DILLIDUR 500 Processing performance

The whole set of processing technology and application technology adopted by the user is very important to the reliability of the products made from this material. It should be ensured that the design, construction and processing methods are suitable for this material, and meet the requirements of the latest processing technology and the purpose of the product that the processor must follow. The user should select the material by himself, and fully consider the high strength and high hardness of the material, and follow the process recommendations that comply with EN 1011-2 (welding) and CEN/TR 10347 (forming), and comply with national regulations for safe production.

3 The approximate conversion value in parentheses is an offensive reference.

Pembentukan sejuk

Although DILLIDUR 500 has high hardness and high strength, it can still be cold formed by bending. It should be noted that as the yield strength increases, the forming force required for the steel plate of the same thickness will also increase, and the resilience will also increase. In order to avoid the risk of edge cracking, the flame cut or sheared edge of the cold bending area should be polished. In addition, it is also recommended to smoothly polish the outer edge of the bend that is subjected to tensile stress during bending.

Semasa pemprosesan, langkah keselamatan yang perlu mesti diambil untuk memastikan kakitangan tidak terdedah kepada bahaya terbang keluar dari bahan kerja semasa pengacuan.

Pembentukan sejuk biasanya boleh mencapai parameter berikut tanpa kecacatan permukaan (t ialah ketebalan plat):

Jejari lenturan minimumLebar bukaan die minimum
Mendatar7 t16 t
Menegak9 t20 t

Kekerasan daripada pembentukan panas DILLIDUR 500 comes from the accelerated cooling of the austenitizing temperature. If the hardness does not decrease significantly after hot forming, it must be supplemented by subsequent re-quenching treatment. However, the hardness obtained after re-quenching will be different from the hardness tested when the steel plate leaves the factory. This is because the cooling efficiency of the quenching equipment in the processing plant is generally lower than that of the quenching equipment during the production of steel plates.

This material can be heated to about 200°C (390°F) without a significant decrease in hardness.

Pemotongan api dan kimpalan
Flame cutting should follow the following minimum preheating temperature: plate thickness 26mm and below, 60°C (140°F);
plate thickness 26~70mm and below, 120°C (248°F); plate thickness above 70mm , 150°C (302°F).

Kimpalan arka manual hendaklah menggunakan elektrod bersalut alkali dengan kelembapan sisa yang rendah (jika perlu, rawatan kering hendaklah dijalankan mengikut keperluan pengeluar elektrod).

Di samping itu, cadangan berikut juga harus dipertimbangkan:

  • For more information on the preheating of DILLIDUR 500, please refer to the technical manual “DILLIDUR-Anti-wear concept”. In any case, preheating above 200 °C (390 °F) must be avoided because it will cause the hardness to decrease (see the figure below).
  • It is best to use low yield strength welding consumables for tack welding, root bead and filler bead. If the welding point needs to withstand wear, only use the wear-resistant welding material that can produce the hardness of the mother board in the last weld pass.

Rawatan haba

DILLIDUR 500The following figure shows the general change in hardness or strength with heat treatment temperature:

Pemesinan

DILLIDUR 500 can use high-speed steel drills, especially cobalt alloy high-speed drills. If the appropriate drilling speed and drilling speed are used, the drill bit can achieve a satisfactory service life.

Keperluan teknikal penghantaran am

Melainkan dipersetujui sebaliknya, teknologi penghantaran am memerlukan penggunaan standard EN 10021.

Toleransi

Melainkan dipersetujui sebaliknya, keperluan toleransi merujuk kepada EN 10029, dan ketebalannya boleh digunakan untuk tahap A.

Kualiti Permukaan

Melainkan dipersetujui sebaliknya, rujuk standard EN 10163-2 dan gunakan tahap A2.

Jumlah nota

Jika terdapat keperluan khas lain untuk bahan yang tidak diliputi dalam dokumen ini kerana tujuan penggunaan atau sebab proses susulan, ia boleh dirundingkan sebelum membuat pesanan.
Kandungan maklumat ini adalah penerangan produk dan mungkin dikemas kini dari semasa ke semasa.
For more detailed information on the application and processing of DILLIDUR 500, please refer to the technical manual “DILLIDUR-Anti-wear concept”.