Metal spinning is used to form a wide variety of high-performance, axially symmetric parts. This metalworking process is compatible with both traditional and exotic metals – such as Inconel. Inconel is ideal for use in some of the toughest conditions found in manufacturing, and is very suitable for applications within high heat, high pressure environments....
X750 is a Nickel-Chromium alloy made precipitation hardenable by additions of Al and Ti, having creep-rupture strength at high temperatures to about 700°C (1290°F). INCONEL® alloy 718 (UNS N07718/W.Nr. 2.4668) is a high-strength, corrosion-resistant nickel chromium material used at -423° to 1300°F. Inconel X750 Inconel X750 Chemical Composition Grade Ni Cr Al C Mn Ti Cu Si S Inconel...
Inconel Inconel is a family of austenitic nickel-chromium-based superalloys. Inconel Composition Inconel Element (% by mass) Ni Cr Fe Mo Nb Co Mn Cu Al Ti Si C S P B 600 72.0 14.0–17.0 6.0–10.0 1.0 0.5 0.5 0.15 0.015 617 44.2–56.0 20.0–24.0 3.0 8.0–10.0 10.0–15.0 0.5 0.5 0.8–1.5 0.6 0.5 0.15 0.015 0.015 0.006...
Grade Incoloy 800/ 800H/ 800HT Incoloy 800 Bolts Specification ASTM B408/ SB408 Nickel Alloy 800 Fasteners International Specifications DIN, ISO, JIS, GB, IS, BS, ASTM and all International Standards Length of Nickel Alloy 800H Bolts 3 – 200 mm Alloy 800 Nuts Sizes M3 – M56 | 3/6″ to 2″ | custom Incoloy 800HT Bolts...
Inconel® is a material that is specifically optimized for some of the toughest use conditions to be found in manufacturing while Duplex stainless steels is the most recent family of stainless steels. They are called duplex (or austenitic-ferritic) grades because their metallurgical structure consists of two phases, austenite (face-centered cubic lattice) and ferrite (body centered...
Hastelloy Hastelloy® is a trademark for a series of high-strength, nickel based, corrosion resistant alloys produced by Haynes International. Alloys of identical chemical and mechanical properties are available from other manufacturers and offer excellent alternatives to the various Hastelloy alloys. FORGING INVENTORY OF NICKEL ALLOYS GENERAL PROPERTIES Density 8.89 gm/cm3 Specific Heat: 427 oC Melting Point...
Nickel base corrosion and temperature resistant alloys are classified as moderate to difficult when machining, however these alloys can be machined using conventional production methods at satisfactory rates. During the machining processes these alloys work harden rapidly, generate high heat during cutting, weld to the cutting tool surface and offer high resistance to metal removal...
Hastelloy C276 is a nickel-molybdenum-chromium superalloy with an addition of tungsten designed to have excellent corrosion resistance in a wide range of severe environments. The high nickel and molybdenum contents make the nickel steel alloy especially resistant to pitting and crevice corrosion in reducing environments while chromium conveys resistance to oxidizing media. The low carbon content minimizes...