4032 (4032-T6, AlSi12.5MgCuNi) Aluminum
4032 aluminum is a 4000-series aluminum alloy. The main alloying addition is silicon. Cited properties are appropriate for the T6 temper. To achieve this temper, the metal is solution heat-treated and artificially aged until it meets standard mechanical property requirements. 4032 is the Aluminum Association (AA) designation for this material. In European standards, it will be given as EN AW-4032. Additionally, the EN chemical designation is AlSi12,5MgCuNi. The British Standard (BS) designation is DTD324B. The AFNOR (French) designation is A-S12UGN. And the UNS number is A94032.
It originally received its standard designation in 1954.
It has the highest tensile strength among the 4000-series alloys in the database.
The graph bars on the material properties cards below compare 4032 aluminum to: 4000-series alloys (top), all aluminum alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it’s 50% of the highest, and so on.
4032 aluminum alloys are known for strong corrosion resistance. 4032 aluminum alloys are sensitive to high temperatures ranging between 200 and 250°C (392 and 482°F), and tend to lose some of its strength. However, the strength of Aluminium/aluminium alloys can be enhanced at subzero temperatures, making them ideal low-temperature alloys.
Chemical Composition:
| Component Elements Properties | Original Value |
|---|---|
| Aluminum, Al | 81.1 – 87.2 % |
| Chromium, Cr | <= 0.10 % |
| Copper, Cu | 0.50 – 1.3 % |
| Iron, Fe | <= 1.0 % |
| Magnesium, Mg | 0.80 – 1.3 % |
| Nickel, Ni | 0.50 – 1.3 % |
| Other, each | <= 0.05 % |
| Other, total | <= 0.15 % |
| Silicon, Si | 11 – 13.5 % |
| Zinc, Zn | <= 0.25 % |
Physical Properties:
| Properties | Metric | Imperial |
|---|---|---|
| Density | 2.69 g/cm3 | 0.0971 lb/in³ |
Mechanical Properties:
| Properties | Metric | Imperial |
|---|---|---|
| Elastic modulus | 70-80 Gpa | 10152-11603 ksi |
| Poisson’s ratio | 0.33 | 0.33 |
Thermal Properties:
| Properties | Conditions | ||
|---|---|---|---|
| T (ºC) | Treatment | ||
| Thermal conductivity | 155 W/mK | 25 | O |
| Thermal expansion | 19.4 x 10-6/ºC | 20-100 | – |
Equivalent Grade:
- Aluminium Association (AA) 4032,
- UNS A94032;
- China GB 4A11 (LD11);
- Japan JIS A4032 (A4×5);
- Canada CSA SG121;
- France NF A-S12UN;
- Britain BS (38S);
- Russia ГOCT 1390 (AK9);
- International ISO 4032
Aluminum 4032 Alloy Health & Safety Information
| Signal Word | N/A |
|---|---|
| Hazard Statements | N/A |
| Hazard Codes | N/A |
| RTECS Number | N/A |
| Transport Information | N/A |
| MSDS / SDS | Request MSDS / SDS |