C95500 Product Introduction Summary

  • Alloy Name: C95500 Nickel-Aluminum Bronze
  • Key Properties: Exceptional strength, corrosion resistance, versatility
  • Composition: Primarily copper, nickel, and aluminum
  • Tensile Strength: 95 ksi
  • Machinability: Bagus sekali
  • Applications: Marine hardware, industrial applications, electrical components, bearings, valves, underwater hardware
  • Compliance: Meets multiple industry standards
  • Shapes and Sizes Available: Comprehensive range for various manufacturing processes
  • Durability: Withstands significant stress and extreme environments
  • Precision Manufacturing: Allows for intricate designs and efficient production
  • Resistance: Exceptional performance in harsh marine environments
  • Longevity: Ensures reliability in demanding applications

Kategori:

Product Introduction

C95500 is a high-performance nickel-aluminum bronze alloy known for its exceptional strength, corrosion resistance, and versatility in various industrial applications. This document outlines the chemical composition, mechanical properties, performance at different temperatures, industry applications, available shapes and sizes, production standards, as well as related standards in different countries.


Komposisi kimia

Table 1: Chemical Composition of C95500

ElemenContent (%)
Copper (Cu)78.00 min
Nickel (Ni)3.00 – 5.50
Aluminum (Al)10.00 – 11.50
Iron (Fe)3.00 – 5.00
Manganese (Mn)≤ 3.50

*Note: The sum of Cu and named elements must be a minimum of 99.5%. Single values represent maximums unless otherwise noted.


Peralatan mekanis

Table 2: Mechanical Properties of C95500

PropertyNilai
Tensile Strength (min)95 ksi (655 MPa)
Yield Strength (min)42 ksi (290 MPa)
Elongation (min)10%
Brinell Hardness (typical)208 BHN

Performance at Different Temperatures

Table 3: Thermal Properties of C95500

PropertyUS CustomaryMetrik
Melting Point – Liquidus1930 °F1054 °C
Melting Point – Solidus1900 °F1038 °C
Konduktivitas listrik8% IACS at 68 °F0.049 MegaSiemens/cm at 20 °C
Konduktivitas termal24.2 Btu/sq ft/ft hr/°F41.9 W/m at 20 °C
Koefisien Ekspansi Termal9 × 10⁻⁶ per °F15.5 × 10⁻⁶ per °C

Industry Applications

Table 4: Typical Uses of C95500

IndustryTypical Uses
Builders HardwareWindow hardware
ConsumerMusical instruments, piano keys
ListrikElectrical hardware
pengencangStuffing box nuts
IndustriAircraft components, bearings, bushings, gears, glands, glass molds, handgun recoil mechanisms, hot mill guides, landing gear parts, machine parts, pickling equipment, piston guides, pump fluid ends, sewage treatment applications, valve bodies, valve components, valve guides, valve seats, wear plates, welding jaws, worms, worms wheels
MarineCovers for marine hardware, marine applications, marine hardware, shipbuilding
ArtileriGovernment fittings

Note: Also available in heat-treated condition.


Available Shapes and Sizes

Table 5: Shapes and Sizes of C95500

Shape/FormUkuran
Solids1/2″ to 9″ O.D.
tabung1 1/8″ to 9″ O.D.*
RectanglesUp to 15″
Standard Lengths144″

*Consult mill for wall thickness.


Production Standards

Table 6: Production Standards for C95500

StandarSpesifikasi
CDAC95500
ASMAB505, B505M
SAEJ461, J462
FederalQQ-C-390, G3
MilitaryMIL-B-16033, Class 4
LainnyaAluminum bronze 9D

Welding and Processing Techniques

Table 7: Welding Techniques for C95500

TeknikKesesuaian
PematerianBagus
mematriAdil
Pengelasan OxyacetyleneNot recommended
Pengelasan Busur Terlindung GasBagus
Pengelasan Busur Logam DilapisiBagus

Table 8: Processing Techniques for C95500

TeknikKesesuaian
Peringkat Kemampuan Mesin50
PemotonganBagus
pemolesanAdil
Perawatan panasEffective

Advantages and Disadvantages

Table 9: Advantages and Disadvantages of C95500

KeuntunganMetode pemotongan
Excellent corrosion resistanceHigher cost compared to alternatives
Good weldabilityComplex processing
Kekuatan tinggiLimited availability in some forms

Similar Products

Table 10: Similar Products to C95500

Similar ProductsKeterangan
C92500Aluminum Bronze alloy
C93200Bearing Bronze alloy
C95400Aluminum Bronze, similar characteristics

Comparison of Similar Products

Table 11: Comparison of C95500 with Similar Products

PropertyC95500C92500C93200
Tensile Strength (ksi)959065
Yield Strength (ksi)423530
Peringkat Kemampuan Mesin506075
Tahan korosiBagus sekaliBagusModerate

Conclusion

C95500 nickel-aluminum bronze is a versatile and durable alloy suitable for a wide range of industrial applications. Its excellent mechanical and thermal properties, alongside compliance with key regulations, make it an ideal choice where strength and corrosion resistance are critical. The information provided in this document can assist engineers and manufacturers in selecting the right materials for their projects.