Standard Specification for Copper Alloy Continuous Castings

ASTM B505 is the premier global standard for copper-base alloys produced by the continuous casting process. This manufacturing method ensures superior material density, uniform grain structure, and high pressure tightness, making these alloys the preferred choice for heavy-duty industrial bearings, bushings, and marine components.


1. Scope of the Standard

The ASTM B505 specification covers continuous cast products in the form of rods, bars, tubes, and shapes. Unlike sand casting (ASTM B148), continuous casting pulls molten metal through a water-cooled graphite die, resulting in a product with virtually no porosity and excellent machinability.


2. Most Common Alloys under ASTM B505

While ASTM B505 covers dozens of copper alloys, the following four represent the majority of global trade and industrial demand:

UNS AlloyCommon NamePrincipal Characteristics
C95400Aluminum Bronze 9CMost popular general-purpose aluminum bronze; high strength and wear resistance.
C95800Alpha Nickel Al-BronzeOptimized for superior corrosion resistance in seawater and brackish water.
C93200SAE 660 Bearing BronzeThe “gold standard” for general-purpose bushings; excellent anti-friction properties.
C86300High Mang. BronzeExtreme high strength and hardness; used for extra heavy loads at low speeds.

3. Chemical Composition (%)

Below are the standard chemical requirements for the two most sought-after Aluminum Bronzes under ASTM B505:

要素C95400 (Aluminum Bronze)C95800 (Nickel Al-Bronze)
83.0 min79.0 min
アルミニウム(Al)10.0~11.58.5~9.5
鉄(Fe)3.0 – 5.03.5 – 4.5
ニッケル(Ni)1.5 max (optional)4.0 – 5.0
マンガン(Mn)0最大.500.8 – 1.5

4. Mechanical Properties (Typical)

Continuous casting enhances the mechanical integrity of these alloys compared to sand-cast equivalents.

財産C95400C95800C93200
引張強さ(分)515 MPa (75 ksi)585 MPa (85 ksi)240 MPa (35 ksi)
降伏強さ (分)205 MPa (30 ksi)240 MPa (35 ksi)140 MPa (20 ksi)
Elongation (in 2″)12%15%10%
Brinell Hardness (Typical)170 HBW150 – 170 HBW70 HBW

5. 物性

財産Value (C95400 / C95800)
密度7.45 – 7.64 g/cm³ (0.269 – 0.276 lb/in³)
融点(液体)1027°C – 1060°C (1880°F – 1940°F)
熱伝導率33 – 59 W/m·K
Coefficient of Expansion16.2 x 10⁻⁶ /K

6. Fabrication & Technical Characteristics

  • 機械加工性: Excellent. Most ASTM B505 alloys provide a smooth finish with high speed-feed rates.
  • 溶接性: Generally good for Gas Shielded Arc Welding (MIG/TIG), particularly for the aluminum bronze series.
  • Non-Sparking: These alloys do not produce sparks upon impact, making them critical for safety tools and equipment in explosive environments (Oil & Gas).
  • Pressure Tightness: The continuous cast process creates a highly dense matrix, ideal for components holding hydraulic fluids or high-pressure steam.

7. Primary Applications

  • Industrial Heavy Machinery: Wear plates, gears, worm wheels, and high-load bushings.
  • Marine Engineering: Seawater pump components, valve bodies, propeller nuts, and marine fasteners.
  • Oil & Gas: Blowout preventer (BOP) parts, drill collars, and non-sparking safety components.
  • Automotive/Transport: Transmission parts and steering mechanisms.

8. Quality Compliance

Material produced under ASTM B505 should be accompanied by a Mill Test Certificate (MTC) confirming:

  1. Full chemical analysis per heat.
  2. Mechanical testing (Tensile, Yield, Elongation).
  3. Dimensional inspection according to standard tolerances.